Surplus lotPrime PBT/PET, 55% glass, from a canceled auto program.120,000 lb PBT/PET 55% glass. See the lot
Plastic resin supply for the U.S. and Canada · Mon–Fri, 8am–5pm ET
Home › Materials › Acetal (POM)

Acetal resin supplier: POM copolymer and homopolymer pellets

We source acetal (POM) copolymer and homopolymer pellets, including high-flow, toughened, low-wear, glass-filled, conductive, UV-stabilized and food-contact grades, in 55 lb (25 kg) bags or from one gaylord (about 1,000 to 1,600 lb) up to truckloads. Send the grade you run, or its type, melt flow at 190°C / 374°F and 2.16 kg and any modifier, and a polymer chemist reviews it and quotes a match or a matched alternative.

Bags or one gaylord to a truckload · Every prime lot from our suppliers ships with a COA

Request a Quote
Shop-floor numbers

Shop-floor numbers

Drying
Usually not needed for standard grades. If damp: copolymer 82–120°C / 180–248°F, 3–4 h · homopolymer 80°C / 176°F, 2–4 h
Melt temp
Copolymer 188–230°C / 370–446°F · homopolymer about 215°C / 419°F
Mold temp
Copolymer 60–121°C / 140–250°F · homopolymer 80 to 100°C / 176 to 212°F
Shrinkage
Copolymer 1.6 to 2.3% · homopolymer 1.7–2.2%
Watch for
Voids and sink in thick sections
Grades
Homopolymer · Copolymer · Low-wear / PTFE-modified · Glass-filled

Typical values; confirm against the grade’s data sheet. Bags or one gaylord to a truckload · Supplier COA on every prime lot · Ships to the U.S. and Canada.

The short answer

Acetal (POM) is the first choice for precision moving parts: gears, cams, clips and pump parts that need stiffness, low friction and steady dimensions in humid air. Pick homopolymer for maximum strength and stiffness, copolymer for hot water, high-pH cleaners and a wider processing window. The thing that most often goes wrong is overheating: acetal held too hot or too long gives off formaldehyde gas, and pressure can build fast in the barrel.

Grades we source

Tap a grade to add it to your quote request.

Never let PVC and acetal meet at processing temperature. Together they can release gas violently. Use separate machines if you can. Otherwise purge with acrylic or a purging compound recommended for the job, then take the injection unit apart and clean the barrel and screw. Never purge PVC with PE or PP.

About Acetal / POM (Polyoxymethylene)

Acetal offers high stiffness and strength, low friction and wear, excellent dimensional stability and good chemical resistance, ideal for moving mechanical parts and precision components. Homopolymer is about 10–15% stronger and stiffer; copolymer holds up better in hot water and in alkaline (high-pH) and chlorinated solutions. POM has a narrow processing window and is attacked by strong acids and oxidizing agents, including chlorinated water over time.

Common applications

  • Gears, cams and bearings
  • Snap-fits and fasteners
  • Fluid-handling and pump components
  • Conveyor and automation parts
  • Precision mechanical components

Typical properties

Impact strengthModerate
Heat (HDT @ 1.8 MPa)~90 to 107°C / 194 to 225°F copolymer · ~93 to 105°C / 199 to 221°F homopolymer (ISO 75, unannealed; Delrin 500P lists 93°C; 25% glass Delrin 525GR about 172°C); continuous use about 80–90°C / 176–194°F
ClarityOpaque
Friction/wearExcellent (low)
Relative costModerate

Property ranges are general guidance and vary by grade and supplier; a polymer chemist reviews the spec against the data sheet and COA.

Full data sheet values: Acetal (POM) properties

Which grade to ask for

Homopolymer or copolymer comes first, then melt flow, then any modifier.

Grade typeUse it forWatch out for
Copolymer, general purposeClips, fasteners, pump and fluid-handling partsModerate notched impact, so radius sharp corners
HomopolymerHighly loaded gears and snap-fits that need the most stiffnessNarrow melt window; less resistant to hot water and alkaline cleaners
High-flow (high melt flow)Thin walls and multi-cavity small partsLess tough than low-flow grades of the same type
Low-wear (PTFE, silicone or other lubricant)Gears running against acetal, conveyor partsLower strength; PTFE is a PFAS
Impact-modified (toughened)Buckles, clips and parts that take impactMust be dried, unlike standard grades; lower stiffness
Glass-filledStiff structural partsGlass reverses the direction of higher shrinkage, so warp changes
Food-contact gradesFood machinery, dispensers, conveyor partsAsk for the producer’s FDA letter for the exact grade and color

Typical starting points. Grades vary, so confirm on the data sheet for the exact grade.

Grade finder: start from what you make

Pick what you make, find the row for your part, and tap Request a Quote to add it to the form. Each row gives the usual type, a typical melt flow window and what to put on the RFQ.

ProductGrade familyTypical windowPut on the RFQQuote
Precision gears and cams under high loadHomopolymer, medium or high viscosityMFR about 2–15 g/10 min (190°C / 374°F, 2.16 kg), lower MFR for tougher, more fatigue-resistant gears; flex modulus about 2.8–3.1 GPa (about 406–450 kpsi)The mating gear, since acetal running on nylon often wears better than acetal on acetal, and whether you need a lubricated grade. Best plastic for gears ›
Gears, rollers and bushings in wet or warm serviceCopolymer, general purposeMFR about 2.5–13 g/10 min (190°C / 374°F, 2.16 kg), with about 9 the common general-purpose flow; flex modulus about 2.5–2.8 GPa (about 363–406 kpsi)Hot water or alkaline cleaners favor copolymer. Ask for the same MFR as your current grade so fill and shrink stay close. Acetal homo vs. copolymer ›
Stiff brackets and structural partsGlass-coupled copolymer or glass-reinforced homopolymer (for example Delrin 525GR, 25% glass), about 10–25% glassMFR where listed (190°C / 374°F, 2.16 kg); glass content by ash (ASTM D5630 or ISO 3451-1)The glass level. Glass changes the shrink pattern and warp, so moving from unfilled acetal is a tool question, not a drop-in. Glass-filled plastics ›
Automotive trim clips, snap-fits and fastenersCopolymer, medium to high flowMFR about 9–27 g/10 min (190°C / 374°F, 2.16 kg)A low formaldehyde emission grade measured by VDA 275, with the limit from your OEM spec, if the part sits inside the cabin, and a UV stabilizer for exposed parts. Plastics for snap-fits ›
Buckles, strap adjusters and parts that take impactImpact-modified (toughened) homopolymer or copolymerMFR about 1–10 g/10 min (190°C / 374°F, 2.16 kg); notched Izod (ASTM D256) several times that of standard grades, with lower stiffnessToughened grades must be dried, about 80°C / 176°F for 4–8 hours to below 0.05%, unlike standard acetal. Plastics for impact ›
Thin-wall, multi-cavity small parts: zipper sliders, pen and cosmetic partsHigh-flow copolymer or homopolymerMFR about 27–50 g/10 min (190°C / 374°F, 2.16 kg)High flow gives up some toughness compared with a lower-flow grade of the same type, so check snap and drop tests. Acetal properties ›
Fuel sender, pump module and fuel cap partsCopolymer fuel grade, sometimes electrically conductiveMFR about 2.5–13 g/10 min (190°C / 374°F, 2.16 kg); conductive grades list volume or surface resistivityThe fuel and temperature (gasoline with ethanol, diesel, biodiesel), the OEM’s fuel exposure test, and whether the part has to dissipate static. Plastics for fuel and oil ›
Pump impellers, valve parts and fittings (not drinking water)CopolymerMFR about 2.5–9 g/10 min (190°C / 374°F, 2.16 kg)The chemical, pH and temperature. Copolymer handles hot water and alkaline cleaners better; strong acids and oxidizers attack both types. Chemical-resistant plastics ›
Conveyor chain, modular belts and sprocketsCopolymer or homopolymer, often lubricatedMFR about 2.5–13 g/10 min (190°C / 374°F, 2.16 kg); low-wear grades with PTFE, silicone or other lubricantsPTFE-free lubricants if your customer restricts PFAS, detectable grades for food lines, and UV stabilizer for outdoor conveyors. Wear and friction fillers ›
Bearings, bushings, slides and wear padsLow-wear homopolymer or copolymerMFR about 2–15 g/10 min (190°C / 374°F, 2.16 kg); friction and wear figures come from each producer’s own test, so compare only like for likeThe mating surface, speed and load, the lubricant type and level, and whether PTFE is allowed. PFAS-free alternatives ›
Inhaler, pen injector and drug-delivery partsMedical-grade copolymer or homopolymerMFR about 9–27 g/10 min (190°C / 374°F, 2.16 kg), by part size and wallThe producer’s medical documents (ISO 10993 or USP Class VI testing where the producer claims it), its change-notification policy, and your sterilization method. Gamma radiation degrades acetal, so EtO is the usual route. FDA and medical grades ›
Instrument handles and reusable device partsCopolymer, often coloredMFR about 2.5–9 g/10 min (190°C / 374°F, 2.16 kg)How many steam autoclave cycles the grade is rated for, and which cleaning chemicals it sees. Copolymer tolerates hot water and steam better than homopolymer. Medical device housings ›
Food-processing machine parts, guides and scrapersFood-contact copolymer, including metal- or X-ray-detectable gradesMFR about 2.5–13 g/10 min (190°C / 374°F, 2.16 kg)The producer’s FDA letter for the exact grade and color (acetal copolymer falls under 21 CFR 177.2470 and homopolymer under 21 CFR 177.2480), EU 10/2011 papers if the equipment is exported, and a detectable grade if the line has metal detection. FDA food contact ›
Faucet cartridges, valve parts and water-meter partsCopolymer listed for drinking waterMFR about 2.5–13 g/10 min (190°C / 374°F, 2.16 kg)An NSF/ANSI/CAN 61 listing for the grade and color at your water temperature, and chlorine or chloramine data, since chlorinated hot water attacks acetal over time. Plastics for hot water ›
Rod, slab and tube stock for machiningLow-flow copolymer or homopolymer extrusion gradeMFR about 1–3 g/10 min (190°C / 374°F, 2.16 kg)An extrusion grade, not a molding grade. Thick homopolymer sections are prone to centerline porosity, which is one reason copolymer is often chosen for thick stock. Acetal homo vs. copolymer ›

These windows are typical published ranges to start the conversation. Acetal flow is measured at 190°C / 374°F and 2.16 kg (ISO 1133 or ASTM D1238). Many sheets give MVR in cm³/10 min instead of MFR in g/10 min; with a melt density of about 1.2 g/cm³, the MFR is roughly 1.2 times the MVR, so check which one the sheet lists before you compare. A chemist checks any alternative before you switch.

Processing notes

  • Drying. Standard copolymer can normally be molded as received; if it has been exposed to moisture, dry at 82–120°C / 180–248°F for 3–4 hours. Standard homopolymer needs drying only above about 0.2% moisture, at 80°C / 176°F for 2–4 hours. Toughened grades must be dried: 4–8 hours at 80°C / 176°F, to below 0.05%. See the drying chart for other resins.
  • Melt temperature. Copolymer 188–230°C / 370–446°F, never above 230°C / 446°F. Homopolymer runs best at about 215°C / 419°F, within the 210 to 220°C / 410 to 428°F range on Delrin sheets. Keep residence short: the Celanese Celcon M90 sheet gives 4 to 10 minutes as optimum and 20 minutes as the maximum, so purge before long stops.
  • Mold temperature. Copolymer 60–121°C / 140–250°F; homopolymer 80 to 100°C / 176 to 212°F. Cold-molded parts keep shrinking in service, and annealing will not rescue a cold-molded homopolymer part.
  • Shrinkage. Copolymer 1.6 to 2.3%, homopolymer 1.7–2.2%. Switching between the two in one tool can change part size.
  • Regrind. Many molders start at 15–25%; copolymer is more forgiving. Never regrind burned, purged or overheated parts.
  • Most common defect. Voids and sink in thick sections, because acetal shrinks so much. Keep hold pressure on until the gate freezes and size gates so they do not freeze early. Mold deposit and a sharp smell mean the melt is too hot or sitting too long.

How acetal prices are set

Acetal starts with methanol. Methanol is made from natural gas, or from coal in much of China. Methanol is oxidized to formaldehyde. For copolymer, formaldehyde is turned into trioxane, which is polymerized with a small share of a comonomer such as dioxolane or ethylene oxide. For homopolymer, purified formaldehyde is polymerized and the chain ends are capped. So methanol and natural gas costs are the main raw-material swing, and the formaldehyde and trioxane steps add energy and conversion cost on top.

Most of the world’s acetal capacity is in Asia, much of it in China, and North America has very few acetal plants. Homopolymer is made by very few companies worldwide. That makes imports matter: ocean freight, exchange rates and import duties on polyacetals (tariff heading 3907.10) all feed into the delivered price. Copolymer usually costs less than homopolymer. Toughened, low-wear, conductive, glass-filled, UV-stabilized and medical grades carry premiums, and PTFE-lubricated grades also depend on PTFE supply and PFAS rules.

Acetal has no monthly industry price settlement like PE and PP. Large buyers usually buy on quarterly or annual contracts with a producer or distributor, producers announce increases by letter, and distributor prices follow with a lag. Chinese market services report a POM price that moves with methanol, but U.S. prices do not follow it one for one. Gulf Coast winter storms, hurricanes and outages at methanol or acetal plants have tightened supply before, and when that happens contract customers are usually served first.

A warning about search results: many acetal price numbers online are per-kilogram figures for Asian markets, market-research estimates or prices for machined rod and sheet. None of them is the price of prime pellets delivered to your dock.

We do not post prices. Every quote is for a specific grade, color, quantity, package and ship-to city. See how resin is priced for the mechanics and the resin market notes for what is moving this month.

What order size does to the price

How you buyTypical sizeWhy the price per pound differs
Truckload of gaylordsAbout 40,000–45,000 lb, about 26–30 boxesClosest to the producer’s or distributor’s best boxed price. Freight per pound is lowest because the truck is full.
Multiple gaylords, LTL or partial truckload2 to about 18 gaylordsFreight per pound runs several times a full truck. Terminal handling, liftgate and fuel surcharges add up.
Single gaylordAbout 1,000–1,600 lbThe highest freight per pound for boxed resin. The seller’s fixed cost of each order (paperwork, COA, credit, handling) is spread over one box.
Bags or a pallet of bags55 lb (25 kg) bags, about 40–55 per palletThe highest price per pound. Common for specialty, colored, medical and imported grades, and for samples and trials.
Bulk truck or railcarBy arrangement onlyRare for acetal. Most acetal, including most truckload volume, ships boxed or bagged.

Freight to your dock, FOB versus delivered terms, imported versus domestic resin, homopolymer versus copolymer and the modifier package can move the price as much as order size, so send your ship-to city with every request.

Ways to lower the cost: buy a full truckload instead of single gaylords, tell us imported resin is OK, or ask about surplus lots and recycled grades if your part allows. See how resin is priced.

Packaging and lead times

PackageTypical net weightNotes
Bag55 lb (25 kg)Common for acetal, especially specialty, colored and imported grades. Often about 40–55 bags per pallet.
Gaylord (box with liner)About 1,000–1,600 lbAcetal pellets are dense, about 48–55 lb/ft³, so the same weight fills a box less deep than PP or PC. Check net weight on the quote and the packing list.
Sealed or barrier bag55 lb (25 kg)Standard acetal can often be molded as received. Toughened grades take up moisture, so keep them sealed until use and dry them anyway.
OctabinAbout 1,000 kg (2,205 lb)Common for imported acetal. Close the liner after every draw.
Bulk truck or railcarBy arrangement onlyRare. Ask only if you run one grade in very large volume and have silos.

Lead time is confirmed with your quote, and we do not promise a ship date until the source has confirmed it. Unfilled copolymer in natural or black at common melt flows usually ships first when it sits packaged in a supplier’s inventory. Homopolymer specialties, toughened, low-wear, conductive, custom-color and medical grades are often made to order on a producer’s or compounder’s schedule, which can take weeks. Imported grades add ocean transit and customs time.

If your drawing names a trademarked grade, send the full grade name. We quote it under that name only when we can source that exact grade through a channel that supports it. Otherwise we quote an acetal homopolymer or copolymer as a similar grade to trial, named as an alternative on the quote, and the drawing owner decides whether it is approved. When acetal goes on allocation, contract customers are served first and lead times stretch for everyone. Tell us the date you need resin on your floor and how much you have on hand. See what to do under allocation or force majeure and gaylord vs. LTL vs. truckload.

What to put on the purchase order

  • Homopolymer or copolymer. They are not drop-in replacements for each other.
  • Melt flow, with its test condition (190°C / 2.16 kg is the usual condition for acetal).
  • Modifiers: low-wear, toughened, UV stabilized, glass-filled.
  • Color: natural (opaque white), black, or a custom match. Black for outdoor parts should be UV-stabilized.
  • Food contact: ask for the producer’s FDA letter for the exact grade. For drinking-water parts, check whether the grade and color are listed to NSF/ANSI/CAN 61 at your water temperature; the finished component is evaluated too.
  • Flame rating: standard acetal is typically UL 94 HB. Recognition is grade-specific and color-specific; check UL Product iQ.
  • COA values: melt flow, plus moisture on toughened grades.

Prime, wide-spec, reprocessed or recycled

MaterialWhat it isWhen it makes senseWhat to ask for
PrimeThe producer’s first-quality resin, in spec, sold under its grade name with a lot COA, in the producer’s packaging.Any part with a drawing callout, an OEM spec, a UL listing, food, water or medical use, or a customer approval.The grade name, homopolymer or copolymer stated, a lot COA with MFR, and the FDA, NSF or UL documents for that grade and color.
Wide-spec or off-gradeMade by the producer but outside the published window, often MFR or color, or transition material. Sold without the grade name.Non-critical parts that tolerate some variation in flow and color.Which property is off and by how much, the MFR measured on each lot at 190°C / 374°F and 2.16 kg, and the type confirmed.
Regrind or reprocessedMolding scrap ground, and sometimes re-pelletized.Your own clean sprues and runners usually go back in at a set share. Each extra heat history adds formaldehyde odor and mold deposit.The source stream, the type, MFR lot to lot, and proof that burned, purged or overheated material was kept out. See using regrind.
PIRPost-industrial recycled: clean manufacturing scrap that never reached a consumer.Recycled content in non-critical parts such as some conveyor and consumer parts.The source process, the type, and whether your customer counts PIR toward its target. See prime vs. off-grade.
PCRPost-consumer recycled acetal. Rare, because acetal parts are small and mixed into other waste.Only where a customer asks for post-consumer content and the part allows variation.MFR window, color, odor and lot data from the recycler. See recycled resin.
Broker or unknown originMaterial with no producer lot number, in plain or re-labeled bags, or sold under a brand name it may not be.Rarely. Homopolymer and copolymer look the same in the bag.The original label and COA. A DSC test shows the melting point, about 178°C / 352°F for homopolymer and about 165°C / 329°F for copolymer. See how to vet a resin supplier.

Checking the COA when the lot arrives

  • Lot number, grade and type. The lot on the COA matches the label on every bag or gaylord, and the grade name and homopolymer or copolymer type match your PO.
  • MFR at 190°C / 374°F and 2.16 kg. The value is inside your window. If the COA lists MVR in cm³/10 min, compare it only with an MVR spec, or convert with care.
  • Formaldehyde, where specified. For automotive interior parts, check the VDA 275 value in mg/kg against your spec, if it has one. VDA 275 holds molded specimens over water in a closed bottle at 60°C / 140°F for 3 hours, so it measures parts, not pellets. On any grade, a sharp smell from a freshly opened bag of new pellets is a warning sign worth a call.
  • Moisture on toughened grades. If the COA lists moisture, check it, and dry toughened grades to below 0.05% before molding no matter what the label says.
  • Modifiers and fillers. Lubricant, UV, conductive or glass content matches the PO. Check glass by ash (ASTM D5630 or ISO 3451-1) and resistivity on conductive grades.
  • Color. Natural acetal is opaque white. Yellowed pellets or brown specks point to heat history.
  • Foreign pellets. Look for any odd pellets in the box. PVC mixed into acetal can release gas violently in a hot barrel, so stop and call if you see any.
  • Keep a retain. Seal a small sample of each lot so you can test it later. See the incoming inspection checklist and what a COA is.

Adding a second source without stopping the line

  1. Write down what you run now. The grade, homopolymer or copolymer, its data sheet, three to six recent COAs with actual MFR values, your mold temperature and process settings, and every approval tied to the grade (OEM spec, FDA letter, NSF listing, UL file, medical file).
  2. Match on paper first. A same-type second source is the easy path. A polymer chemist compares MFR at 190°C / 374°F and 2.16 kg, nucleation, stabilizers, lubricant, impact modifier and documents, and tells you what differs.
  3. Plan for shrink if you change type. Homopolymer is more crystalline and often shrinks slightly more than a copolymer of similar flow, but nucleation, wall thickness and mold temperature can outweigh that, so measure rather than assume. Homopolymer sheets call for about 80 to 100°C / 176 to 212°F, against 60–121°C / 140–250°F for copolymer. A difference of 0.2 points of shrink is about 0.1 mm on a 50 mm part, enough to change gear backlash and snap forces. Measure first articles at least 24–48 hours after molding, since acetal keeps shrinking after it leaves the tool. See switching resin in an existing mold.
  4. Get approvals before volume. Homopolymer to copolymer is a material change and needs requalification. If the drawing names a brand, a substitute needs the drawing owner’s approval, and automotive, NSF, FDA and medical approvals are tied to the exact grade.
  5. Keep the second source active. Buy a small regular volume and trend its COAs, so it is ready if your main grade goes on allocation. See how to qualify a second resin source.

Want a chemist to compare a second source with what you run now? Send the grade and recent COAs through the quote form or an RFQ package.

When to consider something else

  • If parts wear, squeak or crack in wet or fuel service, look at polyketone.
  • If toughness and abrasion resistance matter more than tight tolerances, see acetal vs. nylon.
  • If you are deciding between the two types, see acetal homopolymer vs. copolymer.
  • If the part sees strong acids or chlorinated water, look at PVDF.
  • If the part runs well above 80°C continuous, look at PEEK for wear parts or PBT for electrical parts.

Grade pages: Delrin 500P and Delrin 100P, with close alternatives to qualify.

Named grades in this class

Producer grade pages with data sheet values, the alternatives we would check, and what to confirm before switching.

Named grades with their own page

Typical data, close alternatives to qualify and buying notes for common named grades in this family: Celcon M25 · Celcon M270 · Celcon M90 · Delrin 100P · Delrin 150 · Delrin 500P · Delrin 511DP · Delrin 525GR · Delrin 900P · Duracon M90-44 · Hostaform C9021 · Kepital F20-03. Running a grade that is not listed? Send it and a polymer chemist will check it.

Common questions

Does acetal need to be dried?

Standard grades usually do not. Copolymer can normally be molded as received, and homopolymer needs drying only above about 0.2% moisture. Toughened grades are the exception: dry them at about 80°C / 176°F for 4–8 hours.

Is acetal food safe?

Many acetal grades are made for food contact, but compliance belongs to the exact grade and color, not to acetal as a family. Ask for the producer’s FDA letter for the grade you will run, and check that it covers your food type and temperature.

Why does acetal smell when it is molded?

A sharp smell means formaldehyde, released when acetal overheats or sits too long in the barrel. Lower the melt temperature, shorten residence, purge before long stops and vent the tool well. Never let acetal meet PVC in a hot barrel.

Can I switch from acetal homopolymer to copolymer in the same mold?

Often, but expect the part size to change. Copolymer shrinks 1.6 to 2.3% and homopolymer 1.7–2.2%, and homopolymer is a little stiffer and stronger. Check dimensions, snap-fit forces and gear backlash on first articles.

What is the price of acetal per pound?

We do not post a price because there is no single one. Acetal follows methanol and natural gas costs, imports and contract terms, and your price also depends on homopolymer or copolymer, the modifier package, color, quantity, packaging and freight. Copolymer usually costs less than homopolymer. See the resin market notes for direction, and send your grade, quantity and ship-to city for a firm quote.

What is the minimum order for acetal pellets?

One gaylord, about 1,000 to 1,600 lb, or the same weight in 55 lb bags for grades that ship bagged. There is no truckload minimum. To qualify a production grade, ask about a sample of about 50 lb, available upon credit approval. If you need machined rod or sheet rather than pellets, a plastics stock-shape distributor is the right source.

Can you supply Delrin pellets?

Delrin is a registered trademark of its owner for its acetal homopolymer, and machinists often use the name for any acetal. If your drawing calls for that exact grade, send the full grade name, and we quote it under that name only when we can source that grade through a channel that supports it. Otherwise we quote an acetal homopolymer from another producer, or a copolymer, as a similar grade to trial, named as an alternative on the quote, and the drawing owner decides whether it is approved.

How much acetal regrind can I use?

Many molders start at about 15–25% clean, same-grade regrind, and copolymer is more forgiving than homopolymer. Each trip through the barrel adds heat history, which shows up as more formaldehyde odor, mold deposit and color shift. Never regrind burned, purged or overheated parts, and keep regrind dry and free of other resins. See regrind limits by resin.

Which acetal is used for fuel system parts?

Copolymer is the usual choice, because it holds up better to hot fuel and hot water than homopolymer. Fuel pump modules and sender parts often use a fuel-grade copolymer, and parts that must dissipate static use a conductive grade. Confirm resistance to your fuel blend and temperature with the OEM’s test. See plastics for fuel and oil.

Related pages (15)

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. We check it, and suggest a matched alternative if it is hard to get.
  3. We aim to quote within one to three business days, from one gaylord to a railcar.
Rather talk? Call (678) 310-6899 or text a photo.
Quote request · Acetal (POM)

Tell us the Acetal (POM) grade you run now

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

Not sure? Just tap through 4 questions4 quick questions, then a chemist suggests a short list.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote