Surplus lotPrime PBT/PET, 55% glass, from a canceled auto program.120,000 lb PBT/PET 55% glass. See the lot
Plastic resin supply for the U.S. and Canada · Mon–Fri, 8am–5pm ET
Home › Materials › PETG
Material

PETG copolyester resin: clear extrusion, sheet and injection grades

For sheet extruders, thermoformers, blow molders and injection molders of clear parts. We quote prime PETG by producer grade, and recycled or regrind PETG, through our supply partners, case by case, from one gaylord where the grade is available. A polymer chemist reviews every request and tells you plainly if we can’t source it.

Request a Quote

The short answer

PETG is a glycol-modified PET copolyester. Part of the ethylene glycol in PET is replaced with a second glycol, usually cyclohexanedimethanol (CHDM), and that stops the polymer from crystallizing. The result is an amorphous, clear resin that stays clear in thick sections, thermoforms and molds easily, and is tougher than standard PET in a notched impact test, about 101–105 J/m against 40–56 J/m. The trade-off is heat. Its glass transition is about 80°C / 176°F, and heat deflection is about 62–64°C / 144–147°F at 1.82 MPa. It fits clear sheet and thermoformed packaging, displays, medical device packaging, extrusion blow molded bottles, heavy-wall jars and clear molded parts. It does not fit parts that see boiling water, a commercial dishwasher or steam sterilization.

What we source

Each quote is for a specific grade or lot through our supply partners, and availability changes.

Supply typeWhat it isWhere it fitsSend us
Prime extrusion and sheet gradesGeneral-purpose PETG for sheet, film, profiles and extrusion blow molding. Eastman Eastar 6763 is one widely used example, and SK chemicals sells PETG as Skygreen.Sheet for blisters, clamshells, trays and medical packaging, displays and signs, profiles, tubing and bottlesThe producer grade name, your process, and clear or tinted
Prime injection gradesPETG for clear molded parts, often with a mold release added. Eastar GN007 is one example.Cosmetic jars and caps, covers, housings and consumer goodsThe grade name, mold release or not, and wall thickness
Recycled PETGPETG repelletized from sheet skeleton, edge trim or molded scrap, where a supply partner has a suitable stream.Colored or opaque sheet, core layers and parts where color and clarity can varyThe grade it must run with, color, and what contamination you can accept
Regrind and wide-specGround sheet trim or parts, and producer lots outside the grade’s window, sold without the grade name.Non-critical sheet and molded partsSource grade if known, color, fines, and limits on PET and PVC

Send the producer grade name. PETG is specified by the producer’s grade, not by the IV windows used for bottle PET. Grades differ in flow, mold release and food or medical paperwork. If your grade is hard to get, a polymer chemist can suggest a similar grade to trial and tells you what differs. PCTG and higher-heat copolyesters are different products, quoted the same way.

Typical properties

PropertyExtrusion grade (Eastar 6763)Injection grade (Eastar GN007)Test
Specific gravity1.271.27ASTM D792
Tensile stress at yield50 MPa50 MPaASTM D638
Flexural modulus2,100 MPa2,060 MPaASTM D790
Notched Izod, 23°C / 73°F101 J/m105 J/mASTM D256
Notched Izod, −40°C / −40°F37 J/m40 J/mASTM D256
HDT at 0.455 MPa70°C / 158°F70°C / 158°FASTM D648
HDT at 1.82 MPa64°C / 147°F62°C / 144°FASTM D648
Glass transitionAbout 80°C / 176°FNot listedDSC
Water absorption, 24 h0.13%Not listedASTM D570
Mold shrinkageNot listed0.2–0.5%ASTM D955
Haze and total transmittance0.8% and 91% (250-micron film)0.2% and 90%ASTM D1003

Typical values from Eastman’s technical data sheets for Eastar copolyester 6763 and Eastar GN007, read in November 2026. Grades from other producers differ a little. Confirm on the data sheet for your grade.

Drying and processing

PETG must be dried, and at a much lower temperature than PET. PET chips are crystalline, so they stay hard in a dryer at 149–171°C / 300–340°F. PETG does not crystallize, so its pellets start to soften and stick together below its glass transition of about 80°C / 176°F.

  • Dryer settings. A desiccant dryer at about 65°C / 150°F. For Eastar 6763, Eastman lists 4 to 6 hours at 65°C / 150°F and says drying must be no higher than 65°C to keep pellets from sticking. Some grades allow slightly more, such as 6 hours at 71°C / 160°F on the GN007 sheet; go higher only where your grade’s own data sheet lists it. Eastman’s injection guide asks for at least 6 hours with air at a dew point of −29°C / −20°F or lower, and warns that pellets may stick together above 70°C / 160°F.
  • Moisture target. Under 0.05% (500 ppm) at the time of melting, per Eastman’s processing guide for amorphous copolyesters. Wet PETG hydrolyzes in the melt, which costs toughness and shows as bubbles or splay.
  • Melt temperature. 249–271°C / 480–520°F on the injection data sheets. Extrusion blow molding runs cooler, about 195–220°C / 383–428°F for Eastar 6763. For sheet, follow the producer’s extrusion guide for your grade.
  • Mold temperature. 16–38°C / 60–100°F. Eastman advises against molds above 55°C / 131°F because parts can stick.
  • Thermoforming. Eastman lists a sheet temperature of about 138–149°C / 280–300°F for Eastar 6763, with the mold surface at about 40–60°C / 104–140°F.

From Eastman data sheets and processing guides. Other producers’ grades can differ, so the guide for your exact grade comes first. See the resin drying guide for other resins.

PETG vs. APET, polycarbonate and acrylic

PropertyPETGAPET (amorphous PET)PolycarbonateAcrylic (PMMA)
ClarityAbout 88–91% light transmission. Stays clear in thick sectionsAbout 88–90%. Thick or slowly cooled sections can crystallize and hazeAbout 88–90%About 92%, the best optics
Impact (notched Izod)Good, about 101–105 J/mLower as molded, about 40–56 J/m. Tough in bottles and filmVery high, about 600–900 J/mLow, about 16 to 21 J/m
Heat (HDT at 1.8 MPa)About 62–64°C / 144–147°FAbout 62–65°C / 144–149°F when amorphousAbout 124–132°C / 255–270°FAbout 76–102°C / 169–216°F
Chemicals and stress crackingUnstressed parts resist dilute acids and bases, alcohols and many oils. Alcohols can craze stressed or thermoformed parts. Ketones and aromatic or chlorinated solvents attack itGood with oils and many solvents. Strong bases and hot water attack itAmmonia, caustic, ketones and many solvents attack it, and it stress-cracksAlcohols, ketones and many solvents craze it
FormingThermoforms easily and does not crystallizeForms well in thin sheet, and must be dried hot before extrusionNeeds higher melt and forming temperaturesForms and machines well, but cracks rather than yields
Outdoor useFair. UV grades for outdoorsFairYellows unless UV-stabilizedExcellent
Relative costModerateLowModerate to highModerate

General comparison of typical clear grades, not prices. Individual grades vary. See unfilled PET, polycarbonate, polycarbonate vs. acrylic and clear plastics compared.

Sterilization and food contact

  • Sterilization. Eastman’s data sheet for Eastar 6763 lists ethylene oxide, gamma radiation and electron beam, with no property loss or color shift when done properly. Steam is not on that list, and it runs well above PETG’s glass transition, so parts distort. Confirm the method in the producer’s statement for your exact grade.
  • Food contact. PETG-type copolyesters usually fall under FDA 21 CFR 177.1315, but food-contact status belongs to the specific grade and its producer’s letter, with its limits on food type and temperature. Ask for the letter for the exact grade. A prime grade’s letter does not carry over to recycled or regrind material. For Canada, Health Canada issues its own letter of no objection on request.
  • Medical. Some grades carry a producer statement on ISO 10993 or USP Class VI testing. Ask for the statement for your grade. The finished article is the manufacturer’s responsibility.

Recycling and regrind

Keep PETG scrap and regrind separate from PET. In a PET dryer, PETG softens and sticks the load together. Check incoming PET flake and regrind for it too.

The recycling industry guidance is specific. The Association of Plastic Recyclers (APR) design guide for PET packaging rates a base resin that melts at 225–255°C as preferred, and treats a resin outside that range, or one that will not crystallize, as not recyclable in the PET stream. Standard PETG does not crystallize, so it falls in that group. California law also defines PET for resin code 1 labeling by composition and the same melting range, which standard PETG does not meet.

That guidance is about the PET bottle and thermoform stream. It does not mean PETG cannot be reused: clean PETG scrap from one known source is reground and run again, and that is the recycled and regrind PETG we quote. See using regrind.

What to put on the request

  • The producer grade name, from the bag label, COA or data sheet.
  • Process. Sheet or film extrusion, extrusion blow molding or injection molding.
  • Supply type and color. Prime, recycled or regrind, and clear, tinted or opaque.
  • Documents. The lot COA, and the food-contact or medical statement if you need one.
  • Quantity and ship-to. This order, yearly use and the city. Our RFQ package page lists what helps a chemist check a match.

Common questions

What is PETG?

PETG is PET modified with a second glycol so that it cannot crystallize. It is an amorphous, clear copolyester used for sheet, thermoformed packaging, displays, bottles, jars and clear molded parts. It is tougher than standard PET in a notched impact test, and it softens at a lower temperature, with a glass transition of about 80°C / 176°F.

Is PETG the same as PET?

No. PET is semi-crystalline, is bought by intrinsic viscosity and dries at 149–171°C / 300–340°F. PETG is amorphous, is bought by producer grade and dries at about 65°C / 150°F. They cannot be swapped for each other, and PETG must be kept out of PET regrind. See unfilled PET and PET and PBT.

What temperature do you dry PETG at?

About 65°C / 150°F in a desiccant dryer for 4 to 6 hours on the Eastar 6763 data sheet, and Eastman says no higher than 65°C for that grade. Some grades allow slightly more, such as 71°C / 160°F for 6 hours on the GN007 injection sheet; use a higher setting only where your grade’s own sheet lists it. The target is under 0.05% moisture. Do not raise the temperature to save time: Eastman warns that pellets may stick together above 70°C / 160°F.

Is PETG food safe?

It depends on the grade. Many PETG grades are sold for food contact, and PETG-type copolyesters usually fall under FDA 21 CFR 177.1315. Compliance belongs to the specific grade and its producer’s letter, with any limits on food type and temperature, so ask for the letter for the exact grade. Recycled and regrind PETG need their own paperwork.

Can PETG be recycled with PET bottles?

It should not be mixed with them. PETG softens and sticks at PET drying temperatures. The APR design guide for PET packaging treats a base resin that will not crystallize as not recyclable in the PET stream, and standard PETG does not meet the California definition of PET for resin code 1. Clean PETG scrap kept on its own can be reground and reused.

Can you quote PETG, and what is the minimum?

Yes. We quote prime, recycled and regrind PETG through our supply partners, case by case, for buyers in the U.S. and Canada. The minimum is one gaylord, about 1,000 to 1,600 lb. Send the producer grade name and quantity, and a polymer chemist will tell you plainly whether we can source it. We aim to quote within one to three business days.

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. A polymer chemist checks it, and suggests a similar grade to trial if yours is hard to get.
  3. We aim to quote within one to three business days, from one gaylord.
Rather talk? Call (678) 310-6899 or text a photo.

Tell us the PETG grade you run now

A polymer chemist reviews every request, then quotes what you asked for or suggests a similar grade to trial.

Optional requests

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The producer grade name, or a data sheet
  • Process: sheet, blow molding or injection
  • Prime, recycled or regrind, and clear or colored
  • Food-contact or medical statement, if you need one
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote