Surplus lotPrime PBT/PET, 55% glass, from a canceled auto program.120,000 lb PBT/PET 55% glass. See the lot
Plastic resin supply for the U.S. and Canada · Mon–Fri, 8am–5pm ET
Home › Materials › PET (unfilled)
Material

Unfilled PET resin: bottle, sheet, fiber and strapping grades, rPET and regrind

For bottle, sheet, fiber and strapping plants and the buyers who source their resin. We quote prime PET by IV, recycled PET pellets and flake, and regrind or wide-spec lots through our supply partners, case by case, from one gaylord where the material is available. A polymer chemist reviews every request and tells you plainly if we can’t source it.

Request a Quote

The short answer

Unfilled PET (polyethylene terephthalate) is the polyester used for bottles, clear sheet, fiber, film and strapping. It is bought by intrinsic viscosity (IV), which tracks chain length: about 0.60–0.68 dL/g for fiber and film, 0.72–0.86 for bottles, 0.76–0.84 for sheet and often 0.80–0.95 for strapping. Cooled fast, it stays amorphous and clear. Held hot, it crystallizes and turns white. It must be dried to about 50 ppm moisture before melting, and amorphous chip, flake or regrind must be crystallized before it goes into a hot dryer. For glass-filled PET molding grades, see PET and PBT.

What we source

We quote three supply types through our supply partners. Each quote is for a specific grade or lot, and availability changes.

Supply typeWhat it isWhere it fitsSend us
Prime (virgin) PETThe producer’s first-quality resin, sold under its grade name with a lot COA. Bottle and sheet chips ship crystallized. Fiber and film chips are often amorphous.Bottles and preforms, APET sheet and thermoforms, staple fiber and filament, strapping and monofilamentThe grade name, or the IV window with its test method, and the end use
Recycled PET (rPET) pelletsPost-consumer (PCR) or post-industrial (PIR) PET that has been melt-filtered and pelletized, sometimes solid-stated to raise IV.Bottles and sheet with recycled-content targets, strapping and fiberIV range, color, food contact or not, and the recycled share you need
rPET flakeWashed, ground bottles or thermoforms. It skips pelletizing and melt filtration, so it costs less, with lower bulk density, more fines and moisture, and unfiltered contamination.Sheet, strapping and fiber lines with good drying, feeding and filtrationClear, light blue, green or mixed, your PVC limit, and the bulk density your feeder needs
Regrind and wide-specRegrind is ground industrial scrap such as preforms, sheet skeleton or edge trim. Wide-spec is made by a producer but outside its window, often on IV, color or acetaldehyde, and sold without the grade name.Sheet core layers, strapping, fiber and non-food parts that tolerate variation. A food-contact sheet with a regrind core behind a virgin barrier layer still needs paperwork covering those use conditionsSource, form, IV range, color, and whether it is crystallized or amorphous

More on recycled streams is on the recycled resin page. Have prime, regrind or obsolete PET to move? See sell surplus resin.

Grades by IV

End useTypical IV, dL/gUsual chip form
Staple fiber, textile filament and BOPET filmAbout 0.60–0.68Melt-phase chips, often amorphous
Water and general beverage bottlesAbout 0.72–0.80Solid-stated copolymer, crystallized
Carbonated soft drink bottlesAbout 0.80–0.86Solid-stated copolymer, crystallized
APET sheet, clamshells and traysAbout 0.76–0.84Bottle or sheet grade, crystallized, often blended with rPET
Strapping and monofilamentOften about 0.80–0.95High-IV virgin, or recycled flake upgraded by solid-state polymerization

Typical published windows. Hot-fill, 5-gallon, CPET and industrial yarn windows, and glass-filled grades, are in the full grade finder by IV. Test methods are on PET grades by intrinsic viscosity.

What to specify

  • IV and its test method. Target, tolerance and the method: ASTM D4603, ISO 1628-5 (as viscosity number) or the producer’s own. Compare suppliers on one method.
  • Clear or colored. Color as L* and b* for chips, or the tint for flake. For bottles, also the acetaldehyde limit.
  • Crystallized or amorphous chip. Crystallized chips are opaque white and can go straight into a hot dryer. Amorphous chips are clear and need a crystallizer first.
  • Pellet or flake, and bulk density. Flake is much lighter than crystallized pellets and varies lot to lot, so ask for the bulk density if your feeder and dryer are sized for pellets.
  • Food-contact paperwork. For prime resin, ask for the producer’s food-contact compliance letter for the exact grade. For post-consumer recycled PET, buyers usually ask for the recycler’s FDA letter of no objection (NOL) for its process. It is FDA’s informal opinion on a process for stated conditions of use, not a regulation or an approval of each lot, so check that the conditions cover your food type, temperature and recycled share. For Canada, Health Canada issues its own letter of no objection on request.

Typical properties

PropertyTypical valueCondition
Density, amorphous1.33–1.34 g/cm³APET sheet. Injection grades list 1.32–1.33
Density, crystallized pellets1.39–1.40 g/cm³Chips as shipped for bottles and sheet
Melting pointAbout 240–250°C / 464–482°FCopolymer bottle grades. Homopolymer grades melt higher
Tensile strength at yield57–58 MPaAmorphous, injection molded, ASTM D638
Flexural modulus2.4–2.5 GPaAmorphous, ASTM D790
Notched Izod impact40–56 J/mAmorphous, 23°C / 73°F, ASTM D256
Heat deflection (HDT)62–65°C / 144–149°F at 1.82 MPa
66–69°C / 151–156°F at 0.455 MPa
Amorphous, ASTM D648
Water absorption, 24 h0.1–0.19%ASTM D570
Mold shrinkage0.2–0.4%Amorphous, cold mold, ASTM D955
Light transmissionAbout 88–90%Clear amorphous sheet and bottle walls. Thicker molded plaques read lower

Typical values. The mechanical and thermal rows are for amorphous PET molded in a cold mold, from three Eastman Eastar data sheets (EN001, EN052 and EN058). Stretch-blown bottle walls, oriented film, fiber and crystallized PET differ. Confirm on the data sheet for your grade.

Drying and processing notes

  • Moisture target. About 50 ppm (0.005%) before melting. Wet PET hydrolyzes in the melt: IV drops, and the product can look fine and still be weak.
  • Dryer settings. A desiccant dryer for 4 to 6 hours (6 preferred), with air entering the hopper at about 149–171°C / 300–340°F so the pellets reach 149–166°C / 300–330°F, and a dew point of −40°C / −40°F or lower. Check the producer’s maximum: one bottle-grade data sheet sets an absolute limit of 180°C / 356°F on dryer air to avoid discoloration.
  • Crystallize amorphous material first. Amorphous chip, clear regrind and flake from sheet or preforms soften at around 80°C / 176°F and clump in a hot dryer. Crystallize with agitation, then dry. Clear regrind is amorphous. Regrind that turned white from heat is crystalline, but white-pigmented regrind can still be amorphous, so ask or test a handful before loading a hot dryer. Crystallizing is not drying.
  • Melt and mold temperature. Injection data sheets for unfilled PET list a melt of about 275–295°C / 527–563°F and a cold mold, 10–30°C / 50–86°F, to keep parts and preforms clear.
  • Recycled and regrind. Washed flake can arrive much wetter than virgin chips, so it needs longer drying.

General practice from producer guides and our resin drying guide. The data sheet for your exact grade comes first.

PET vs. PETG vs. PBT

PropertyPET (unfilled)PETGPBT (unfilled)
StructureSemi-crystalline. Clear only when cooled fast or orientedAmorphous. Stays clear in thick sectionsSemi-crystalline. Opaque, crystallizes fast
Density1.32–1.34 g/cm³ amorphous1.27 g/cm³1.30–1.31 g/cm³
Notched Izod40–56 J/m101–105 J/m30–60 J/m
Drying149–171°C / 300–340°F to about 50 ppmAbout 65°C / 150°F to under 0.05%About 121°C / 250°F to 0.02%
Main usesBottles, sheet, fiber, film and strappingClear sheet, displays, medical packaging, jarsConnectors and electrical housings
Read moreThis pagePETG copolyesterPET and PBT, PBT vs. PET

Typical values for unfilled grades. The three are not interchangeable: PETG softens and sticks in a PET dryer, and PBT is mainly an injection molding resin.

Buying checklist for recycled and regrind lots

  • Source and form. Post-consumer bottles or thermoforms, or post-industrial scrap such as preforms or sheet skeleton. Flake, regrind or pellets. One source or a blend.
  • IV and its spread. IV by a stated method, with the range lot to lot. Bottle flake often arrives at about 0.70–0.80 dL/g, and green or mixed flake for fiber and strapping at about 0.65–0.78. Expect a wider spread than virgin.
  • Color. Clear, light blue, green or mixed, with L* and b* and a black speck limit if the product is clear.
  • Contamination. Limits in ppm for PVC, PETG, polyolefin from caps and labels, adhesive, paper and metal. One PVC chip can burn in the melt or break a fiber, and PETG softens and sticks at PET drying temperatures.
  • Moisture and crystallinity. Moisture as delivered, and whether the lot is crystallized or amorphous, which decides whether you need a crystallizer.
  • What the paperwork shows. Prime lots come with a producer COA. Regrind and wide-spec often come with a test report instead. Check which tests were run, by what method, and whether the results are for this lot or typical. See what a COA shows.
  • Trial first. Run one gaylord before you commit to volume. See processing recycled resin.

What to put on the request

  • Supply type and end use. Prime, recycled pellets, flake, regrind or wide-spec, and the product it goes into.
  • IV window and method, plus form (crystallized or amorphous, pellet or flake) and color.
  • Documents. The lot COA or test report, and the food-contact letter if you need one.
  • Quantity, packaging and ship-to. This order, yearly use and the city. Bottle and fiber PET is mostly sold by bulk truck and railcar, so a gaylord costs more per pound. See the RFQ package page.

Common questions

What is unfilled PET used for?

Bottles and preforms, clear APET sheet for thermoformed clamshells and trays, staple fiber and filament, BOPET film, and strapping. Each use runs in its own IV window, from about 0.60–0.68 dL/g for fiber and film to about 0.80–0.95 for strapping. Glass-filled PET for molded parts is a different product.

What is the difference between PET and PETG?

PETG is PET modified with a second glycol so that it cannot crystallize. It stays clear in thick sections and is tougher in a notched impact test, but it is specified by producer grade, not by bottle IV windows, and it dries at about 65°C / 150°F, not at PET temperatures. The two cannot be swapped for each other, and PETG must be kept out of PET regrind.

How dry does PET need to be?

About 50 ppm (0.005%) moisture before melting, usually reached with dryer air at about 149–171°C / 300–340°F for 4 to 6 hours with air at a dew point of −40°C / −40°F or lower. Measure moisture after the dryer, because the right setting depends on throughput and hopper size.

Why does PET regrind or flake stick in the dryer?

Because it is amorphous. Clear PET regrind and flake from sheet or preforms soften at around 80°C / 176°F and fuse into clumps at PET drying temperatures. Crystallize it first with agitation, then dry it. Material that turned white from heat is crystallized and does not need this step, but white-pigmented regrind can still be amorphous.

Can recycled PET be used for food packaging?

It can be, with paperwork that covers the use. For post-consumer rPET, buyers usually ask for the recycler’s FDA letter of no objection and check that its conditions, such as food type, temperature and recycled share, cover their use. That letter is FDA’s informal opinion on a recycling process for stated conditions of use. It is not a regulation and not an approval of each lot, and it is not the only route: FDA’s recycling guidance treats in-plant scrap and recycled layers behind a virgin PET barrier separately. For Canada, Health Canada issues its own letter of no objection on request. The finished package remains the manufacturer’s responsibility.

Can you quote prime, recycled and regrind PET?

Yes. We quote all three through our supply partners, case by case, for buyers in the U.S. and Canada. The minimum is one gaylord, about 1,000 to 1,600 lb of pellets. A gaylord of flake or regrind weighs less. Send the grade or IV, the form and the quantity, and a polymer chemist will tell you plainly whether we can source it. We aim to quote within one to three business days.

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. A polymer chemist checks it, and suggests a similar grade to trial if yours is hard to get.
  3. We aim to quote within one to three business days, from one gaylord.
Rather talk? Call (678) 310-6899 or text a photo.

Tell us the PET you run now

A polymer chemist reviews every request, then quotes what you asked for or suggests a similar grade to trial.

Optional requests

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or the IV with its test method
  • Prime, recycled pellets, flake, regrind or wide-spec
  • Crystallized or amorphous, and clear or colored
  • Food contact or not, and the letter you need
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote