Resin sourcing for blown and cast film converters
Stretch and shrink film, can liners, bags, sacks, ag film and laminating webs. We source LLDPE (butene, hexene, octene and metallocene), LDPE, HMW-HDPE, MDPE, EVA, plastomers and cast PP by melt index, density and comonomer, plus the slip, antiblock, processing aid, color and PCR that go into your blend.
Request a QuoteHow we help film converters
Film converters feel resin variation right away. A small shift in melt index or density changes bubble stability, frost line height, gauge and sealing, and a lot with high gels turns into rejected rolls. Most lines run blends and coextruded structures, so a gap in one LLDPE, one LDPE or one slip concentrate stops the whole recipe. You buy by the hopper car, bulk truck and contract release, and a force majeure or allocation notice from one producer can leave you a few weeks from running out.
Send us the grade name, or the MI, density, comonomer, catalyst type and additive package for each resin in your blend. A polymer chemist reviews every request and matches the grade you run now or a matched alternative, and tells you plainly what will differ, then we quote it. We quote contract and release volumes from one gaylord of concentrate up to truckload and railcar, shipped to your plant, and every prime lot from our suppliers ships with a COA. Development samples are available upon credit approval when you are qualifying a new blend or a second source.
Materials we source for this industry
- LLDPE: butene (C4), hexene (C6) and octene (C8) film grades, fractional to about 4 MI; see butene vs. hexene vs. octene
- Metallocene LLDPE and plastomers (POP/POE): down-gauging, sealant and cling layers
- LDPE: fractional-melt shrink grades, clarity grades and extrusion coating grades; see LDPE blown film resin
- HMW-HDPE and MDPE: thin-gauge high-strength bags, liners and stiff sack layers
- EVA by vinyl acetate content: freezer film, sealant, cling and ag film; see EVA by VA, 18% VA EVA grades and EVA film grades
- Polypropylene: cast film homopolymer and random copolymer for clarity and sealing
- Additive concentrates: slip, antiblock, processing aids (fluoropolymer and PFAS-free), UV and antistat
- Color concentrates: white, black and custom colors for bags, liners and ag film
- Recycled PE (PCR / PIR): film-grade pellets for blending into liners, sacks and stretch film; for trash bags and film blends that can take some variation, see wide-spec polyethylene
- PBAT: compostable film blends for bags and liners
- Named film grades with their own pages: DOWLEX 2045G, DOWLEX 2047G, Exceed 1018, ExxonMobil LL 1002, NOVAPOL PF-0218-F, Petrothene GA502024, Petrothene NA952000 and DOW LDPE 640I
Typical products and the resins behind them
| Film product | Typical resins | What drives the choice |
|---|---|---|
| Cast stretch wrap (hand and machine) | Hexene, octene and metallocene LLDPE at about 2–4 MI; cling skin from a plastomer, VLDPE or EVA | Ultimate stretch, puncture and load holding at the gauge you run; cling level and noise on unwind. |
| Shrink and bundling film | Fractional-melt LDPE (about 0.2–0.8 MI) blended with LLDPE or mLLDPE | Shrink force and melt strength from LDPE, toughness and puncture from LLDPE; bubble stability on your die. |
| Can liners and trash bags | Butene LLDPE for economy grades, hexene or mLLDPE for premium, HMW-HDPE for thin high-strength bags, PCR | Dart and tear at the target gauge; some states set minimum post-consumer content for trash bags. |
| T-shirt and merchandise bags | HMW-HDPE, sometimes with some LLDPE; white and color concentrates | Strength and stiffness at very thin gauge; handle tear; local bag rules. |
| Lamination and pouch sealant webs | Metallocene LLDPE, plastomers, EVA, LDPE for processing | Seal initiation temperature, hot tack, caulkability, low odor; slip level that does not hurt treat level or lamination bond. |
| Freezer, ice and frozen food bags | Hexene or octene LLDPE, mLLDPE, low-VA EVA | Toughness at freezer temperatures, seal strength, food-contact documents. |
| Agricultural and greenhouse film | LDPE, LLDPE and EVA with UV stabilizer packages | UV life over the seasons the film must last, agrochemical exposure; EVA for clarity and heat retention. |
| Heavy-duty shipping and FFS sacks | LDPE/LLDPE and mLLDPE blends, sometimes an HDPE or MDPE layer for stiffness | Drop strength, stiffness for form-fill-seal machines, hot tack, block resistance. |
| Produce, bakery and clarity bags | Clarity LDPE, mLLDPE, LLDPE blends | Haze and gloss, low gels, sealing; food-contact letters for every resin and concentrate. |
| Cast PP film | PP homopolymer, random copolymer for sealing and clarity layers | Clarity, stiffness and gauge control; random copolymer lowers seal initiation temperature. |
| Compostable bags and liners | PBAT, often blended with PLA or starch | Tear and puncture versus PE, shelf life of the film; finished-product certification is the converter's. |
Typical choices only. Grades within each family vary widely in MI, density, MWD and additives, so confirm properties on the data sheet for the exact grade and trial on your line.
What to specify
Film converters usually specify resin by producer grade name plus melt index, density, comonomer and additive package, then approve it with a line trial and film tests at the gauge they run. When a grade has to change, the spec that matters is the one your line and your customer see: bubble stability, motor load, gels, COF, dart, tear and seal strength. We match against all of it, not just MI and density.
- Melt index, density, comonomer and catalyst. MI under ASTM D1238 at 190°C / 374°F and 2.16 kg; density under ASTM D1505 or D792; comonomer as butene (C4), hexene (C6) or octene (C8); catalyst as Ziegler-Natta or metallocene. Two grades at the same MI and density can differ in molecular weight distribution, so ask for the flow rate ratio (I21/I2 or I10/I2) when matching across producers. See melt flow index.
- HMW-HDPE and MDPE. HMW-HDPE film grades are usually quoted by high-load melt index (190°C / 374°F, 21.6 kg) because their standard MI is too low to read well. Many are bimodal, and two grades at the same HLMI and density can run a different bubble neck height and give different dart. MDPE sits between LLDPE and HDPE in density and is used for stiffness in sacks and liners.
- Gels and lot-to-lot consistency. Ask how gels are measured (often an optical film scanner counting gels per area by size class) and what the limit is. Ask what MI and density ranges the producer releases a lot within, since drift inside spec can still move frost line height and bubble stability. See gels and fisheyes in film and new lot runs differently.
- Additive package. Slip (erucamide or oleamide), antiblock (talc, silica or diatomaceous earth), processing aid, antioxidant and UV stabilizer, either in the base resin or added as concentrates, with type and ppm on the data sheet. Abrasive antiblocks and some pigments can reduce the efficiency of a processing aid. Many buyers now ask for fluorine-free processing aids because of PFAS rules on packaging; see PFAS-free alternatives.
- Slip bloom and COF. Oleamide blooms within hours; erucamide blooms more slowly, over a day or more, but is more heat stable and less volatile. Measure COF under ASTM D1894 at a fixed age (for example 24 hours and 7 days) and roll temperature, because COF keeps moving as slip migrates. Slip on the surface also lowers treat level and can weaken print and lamination bonds.
- Film tests for qualification. Dart impact (ASTM D1709, Method A or B), Elmendorf tear MD and TD (ASTM D1922), tensile (ASTM D882), puncture (ASTM D5748, written for stretch film but widely used), haze (ASTM D1003), gloss (ASTM D2457) and COF (ASTM D1894). Test at the gauge and blow-up ratio you run; downgauging often shows up first as a drop in MD tear or dart. See tearing and puncture.
- Sealing. For sealant layers, specify seal initiation temperature, seal strength (ASTM F88) and hot tack (ASTM F1921). Metallocene LLDPE, plastomers and EVA lower seal initiation temperature; slip, antiblock and contamination in the seal area work against you. See heat seal failures. For acid copolymer and ionomer sealants, see EAA, EMAA and ionomer resin.
- Food contact. Polyethylene and polypropylene are covered by FDA 21 CFR 177.1520 and EVA by 21 CFR 177.1350, and some newer grades rely on a food contact notification (FCN). The producer states compliance for its exact grade under stated conditions of use. Each concentrate needs its own statement, and the finished film is the converter’s responsibility. For the EU, ask for a declaration of compliance under Regulation (EU) No 10/2011, and run migration testing on the finished film where your customer requires it.
- Recycled content. Washington and New Jersey set minimum post-consumer content for plastic trash bags that steps up on fixed dates, and New Jersey’s minimum depends on bag thickness. Rules change, so check the current schedule in each state you ship to. PCR film pellets bring gels, odor and wider MI variation, so ask about melt filtration and devolatilization and start at a low blend level. PCR in food-contact film normally comes from a recycling process with an FDA no-objection letter; the review is voluntary, but many buyers expect it. See processing PCR resin.
Second sources and grade swaps without stopping the line
When a producer declares force majeure or puts a grade on allocation, the fastest fix is a grade you have already trialed. We match on MI, density, comonomer, catalyst, flow rate ratio and additive package (slip and antiblock type and ppm, processing aid, antioxidant), and we tell you where the closest equivalent differs. A hexene grade does not replace an octene or metallocene grade one for one, and a natural grade does not replace a slip and antiblock grade without adjusting your concentrates. See our force majeure plan and backup source program.
To trial a swap without stopping production, run the new grade into one extruder or one layer of a coex line first, stepping its share of the blend up (for example 25%, then 50%, then 100%). Watch motor load, melt pressure and temperature, frost line height, bubble stability, gauge profile and gels at each step, and hold the trial rolls until dart, tear, COF at 24 hours and 7 days, and seal strength pass. Once approved, we can quote contract volume with monthly releases by bulk truck or hopper car to your silo, and gaylords for concentrates and minor blend components.
Guides for this industry
- Gels and fisheyes in film: resin, contamination and process causes and fixes, including PCR gels.
- Blown film bubble instability: melt strength, cooling and blend causes, and what lot drift does.
- Melt fracture and sharkskin: processing aids, die gap and resin choices for mLLDPE and HMW-HDPE.
- Film blocking: slip, antiblock and winding fixes.
- Heat seal failures: sealant resin and process settings that fix weak seals.
- Film tearing and puncture: resin fixes when dart and tear drop after downgauging.
- LLDPE film resin: butene vs. hexene vs. octene: how comonomer changes dart, tear and cost.
- How to qualify a second resin source: the documents and trials that approve an equivalent grade.
Common questions
Why do you ask for comonomer and catalyst as well as melt index and density?
Butene, hexene and octene LLDPE at the same MI and density give different dart, tear and puncture results, with hexene, octene and metallocene grades generally tougher. Metallocene grades also seal at lower temperatures and process differently. A swap can run on your line and still change how the film performs, so we match all four.
Can I replace a Ziegler-Natta hexene LLDPE with a metallocene grade?
Often, but treat it as a requalification. Metallocene LLDPE usually raises dart and lowers seal initiation temperature, but its narrower molecular weight distribution can raise motor load and melt pressure, lower melt strength and bring on melt fracture. Many converters add LDPE or a processing aid, or adjust blend ratios, when they make the change.
Can you match an HMW-HDPE film grade?
Yes. We quote by high-load melt index, density and the gauge you run, and ask whether the grade is bimodal. Bubble stability and dart on your own line are the final test, so trial before you switch.
Do slip and antiblock come in the resin or separately?
Both ways. Some film grades come with slip and antiblock already added, at levels shown on the data sheet, and others are sold natural for you to add concentrates. When you replace a grade, match the additive package or expect changes in blocking, COF and how long the film takes to reach its final COF.
Does an FDA-compliant LLDPE make my bag compliant for food contact?
The producer states compliance with 21 CFR 177.1520 for its grade under stated conditions of use. Colorants, slip and other concentrates need their own statements, and compliance of the finished film is the converter’s responsibility.
If your grade is not listed, tell us what you run. We source commodity, engineering and specialty resins.
Talk to a polymer chemist
Have a grade on a print, a bag label, or just a part you need to make? Send what you have.
- Send the grade, a callout or a photo of the bag label.
- We check it, and suggest a matched alternative if it is hard to get.
- We aim to quote within one to three business days, from one gaylord to a railcar.
Tell us the film grades in your blend
A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.
What to send for an accurate quote
- The grade name, from any supplier, or a data sheet
- Color (natural, black or a custom match)
- Fill type and percentage, if any
- Melt flow, if you know it
- Quantity for this order and what you use in a year
- Ship-to ZIP or postal code