Surplus lotPrime PBT/PET, 55% glass, from a canceled auto program.120,000 lb PBT/PET 55% glass. See the lot
Plastic resin supply for the U.S. and Canada · Mon–Fri, 8am–5pm ET
Home › Materials › PP Homopolymer, Random & Impact Copolymer

PP homopolymer vs. random vs. impact copolymer: which to buy, by MFR

Homopolymer for stiffness, random copolymer for clarity, impact copolymer for toughness, including in the cold. Tell us the type and melt flow rate and we’ll match it.

One gaylord to a railcar · Every prime lot from our suppliers ships with a COA

Request a Quote
Shop-floor numbers

Shop-floor numbers

Drying
Not needed unfilled; if surface moisture shows, follow the grade sheet; filled grades 80 to 82°C / 176 to 180°F, 2 to 3 h
Melt temp
200 to 260°C / 392 to 500°F
Mold temp
10 to 60°C / 50 to 140°F
Shrinkage
Homopolymer 0.8–2.5% · copolymer 1.2–2.0%
Watch for
Stress whitening
Grades
Homopolymer · Random copolymer · Impact copolymer · Talc- and glass-filled PP

Typical values; confirm against the grade’s data sheet. One gaylord to a railcar · Supplier COA on every prime lot · Ships to the U.S. and Canada.

The short answer

Choose homopolymer when stiffness and heat matter, impact copolymer when the part will be dropped or used cold, and random copolymer when it has to be see-through. Melt flow rate then decides which process the grade suits. A common mistake is homopolymer in a part that gets dropped in winter: it passes every test at room temperature and cracks in the field.

Which type of polypropylene?

Polypropylene comes in three families. Homopolymer is the stiffest and most heat resistant, but turns brittle in the cold. Random copolymer adds a little ethylene for better clarity and a lower melting point. Impact copolymer carries a rubber phase that keeps parts tough even below freezing. Within each, melt flow rate (MFR, at 230°C / 2.16 kg) sets the process: low MFR for extrusion and thermoforming, mid MFR for general injection molding, high MFR for thin-wall parts.

Grades we source

Tap a grade to add it to your quote request.

Typical MFR by process

Sheet, thermoforming, extrusion~1–4 g/10 min
General injection molding~10–35 g/10 min
Thin-wall injection molding~35–100+ g/10 min
Fiber and nonwovensWide range, often higher

Homopolymer vs. impact copolymer

StiffnessHomo: higher · Impact: lower
Cold impactHomo: poor · Impact: good
Heat resistanceHomo: higher
ClarityRandom copolymer is best
Density~0.90 g/cm³ (all)

Property ranges are general guidance and vary by grade and supplier; a polymer chemist reviews the spec against the data sheet and COA.

Full data sheet values: Polypropylene density and properties

Which grade to ask for

Pick the type by what the part has to survive, then the melt flow by the process.

Grade typeUse it forWatch out for
Homopolymer, low MFR (about 1–4)Sheet, thermoformed trays, extruded profilesBrittle near 0°C / 32°F. Usually too low in flow for thin-wall injection molding.
Homopolymer, mid to high MFRCaps, living-hinge closures, housewares, fiberNotched Izod typically only 20–55 J/m. Fine for stiff parts, poor for drops.
Clarified random copolymerClear boxes, cups, lids, medical disposablesLower stiffness and heat resistance than homopolymer. Haze rises in thick walls.
Impact copolymer, medium impactPails, crates, battery cases, general industrial partsFlexural modulus about 0.9–1.7 GPa against about 1.1–2.1 GPa for homopolymer (nucleated grades at the top). Whitens at bends.
Impact copolymer, high impactAutomotive interior, cold-storage and freezer containersLower stiffness and heat deflection again. Judge it on impact at the use temperature, not at room temperature.
High-MFR impact copolymer (35 to 100+)Thin-wall tubs and lids that still need some drop resistanceWithin a family, impact usually drops as MFR rises. Run the drop test on the real part.

Typical starting points. Grades vary, so confirm on the data sheet for the exact grade.

Processing notes

  • Drying. None needed for natural, unfilled grades of any type, since PP absorbs very little water. If surface moisture causes splay, follow the drying step on that grade’s data sheet. See the drying chart for other resins.
  • Melt temperature. Homopolymer and copolymer both run about 200 to 260°C / 392 to 500°F on our processing chart, but grade sheets differ, so check the copolymer sheet before you carry a homopolymer setup across.
  • Mold temperature. Homopolymer 10 to 60°C / 50 to 140°F, copolymer 15 to 65°C / 59 to 149°F. For clarified random copolymer, a cooler mold and thinner walls usually give a clearer part.
  • Shrinkage. Homopolymer 0.8–2.5%, copolymer 1.2–2.0% measured 24 hours after molding. The ranges overlap, but a type change in an existing mold can still move critical dimensions. Check first articles. See switching resin in an existing mold.
  • Regrind. 20–30% same-grade regrind is a common start. Keep homopolymer and copolymer regrind apart. Mixed regrind gives a part that is neither as stiff nor as tough as either type.
  • Most common defect: stress whitening. Impact copolymer turns white where it is bent, struck or pushed off the core by ejector pins. Larger radii, more draft and even ejection reduce it. With homopolymer the matching problem is cracking in cold service. See brittle or cracking parts.

What to put on the purchase order

  • The type, in words. Homopolymer, random copolymer or impact copolymer, and for impact copolymer whether it is a medium- or high-impact grade.
  • MFR and its range. Nominal MFR at 230°C / 446°F and 2.16 kg, plus the producer's spec range, so a lot at the edge does not flash or short your mold.
  • Impact at the temperature that matters. Notched Izod at 23°C / 73°F, and for cold service a low-temperature value if the data sheet lists one (for example at −20°C / −4°F or −30°C / −22°F). Compare grades only at the same temperature and test method.
  • Stiffness. A flexural modulus range, so a substitute does not make a lid or crate floppy.
  • Additives. Nucleated, clarified, antistatic or UV-stabilized. A clarified random copolymer and a plain one are not interchangeable.
  • Food or medical use. Ask for the producer's FDA letter for the exact grade. For medical disposables, ask what biocompatibility testing the producer documents. See medical and FDA grades.

When to consider something else

  • If even high-impact copolymer cracks in the cold, look at HDPE: PP vs. HDPE.
  • If you need more clarity or lower extractables than random copolymer gives, look at clear metallocene PP: metallocene PE and PP.
  • If homopolymer is not stiff enough, look at talc- or glass-filled PP: glass-filled vs. mineral-filled.
  • If the part should feel soft or rubbery, look at TPE and TPV.

Common questions

How can I tell if a PP grade is homopolymer or copolymer from the data sheet?

Most sheets say so in the description. If not, look at flexural modulus and notched Izod: homopolymer is the stiffer grade with low impact, typically 20–55 J/m, while impact copolymer is softer with impact that can run from about 60 to 500 J/m. A low-temperature impact value on the sheet is a strong sign of an impact copolymer.

Can I switch from homopolymer to impact copolymer in the same mold?

Usually, yes. Density is about the same and the shrinkage ranges overlap. Match the melt flow, then check critical dimensions, stiffness and fit on first articles, because the copolymer will be softer and may shrink a little differently.

Which polypropylene is best for living hinges?

Most hinge grades are homopolymer or random copolymer at a mid melt flow, gated so the melt flows across the hinge rather than along it. Flex the hinge a few times right after molding while it is still warm. That orients the material and gives a hinge that lasts.

Why does polypropylene turn white when it is bent?

That is stress whitening. Impact copolymer contains a rubber phase, and when the part is strained, tiny voids open around the rubber particles and scatter light. It is mostly cosmetic, but it marks where the part is overstressed. Larger radii, less ejection force or a different impact grade usually help.

Related pages (16)

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. We check it, and suggest a matched alternative if it is hard to get.
  3. We aim to quote within one to three business days, from one gaylord to a railcar.
Rather talk? Call (678) 310-6899 or text a photo.

Tell us the grade you run now

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

Not sure? Just tap through 4 questions4 quick questions, then a chemist suggests a short list.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote