Home › Materials › Clear Polycarbonate

Clear polycarbonate supplier: injection and extrusion grades by melt flow

Clear, tough and heat resistant. We source clear PC from low-flow extrusion grades to high-flow thin-wall and optical grades, plus UV, FDA and flame-retardant versions. Tell us the MFR and Izod you need.

One gaylord to a truckload · Every prime lot from our suppliers ships with a COA

Request a Quote
Shop-floor numbers

Shop-floor numbers

Drying
About 120°C / 248°F, 2–4 h
Melt temp
280–320°C / 536–608°F
Mold temp
70–120°C / 158–248°F
Shrinkage
About 0.5–0.75%, even both ways
Watch for
Black specks and yellowing
Grades
Low-flow grades · Medium- and high-flow injection grades · Optical and lens grades

Typical values; confirm against the grade’s data sheet. One gaylord to a truckload; bulk by arrangement · Supplier COA on every prime lot · Ships to the U.S. and Canada.

The short answer

Clear polycarbonate is for transparent parts that have to survive impact: lenses, light covers, glazing, guards and face shields. Choose it over acrylic when breakage is the risk, and over clear styrenics when you need heat resistance. What most often goes wrong is cosmetic: yellowing, black specks or splay from resin that was degraded, contaminated or not dried to 0.02% moisture or less.

Grades we source

Tap a grade to add it to your quote request.

About clear polycarbonate

Polycarbonate combines glass-like clarity with very high impact strength and good heat resistance. Grades are usually chosen by melt flow rate (measured at 300°C / 1.2 kg): lower MFR for extrusion and the toughest parts, higher MFR for thin walls, long flow paths and optical parts. Typical melt flow (300°C / 1.2 kg): about 10–20 g/10 min for general injection molding; lower for extrusion and the toughest parts; higher for thin-wall parts.

Buyers also specify notched Izod, UV stabilization, release agent, food-contact status and flame rating. Polycarbonate must be dried thoroughly before molding.

Common applications

  • Lenses, light covers and LED diffusers
  • Machine guards and face shields
  • Reusable water bottles (such as large water-cooler bottles) and food-contact containers, where regulations allow. Not for baby bottles or sippy cups; tell us if the part is exported or must be BPA-free.
  • Medical and electronic housings
  • Glazing and sheet

Typical properties

Light transmission~88–90% (clear grades)
Impact strengthVery high
Heat (HDT @ 1.8 MPa)~124–132°C (~136–138°C @ 0.45 MPa)
UVYellows unless UV-stabilized
Scratch resistanceLow uncoated (softer than acrylic); hard-coat for wear surfaces
Relative costModerate-high

Property ranges are general guidance and vary by grade and supplier; a polymer chemist reviews the spec against the data sheet and COA.

Full data sheet values: Polycarbonate density and properties

Which grade to ask for

For clear parts, pick the grade by flow length, optical demands and whether the part sees sunlight.

Grade typeUse it forWatch out for
Low-flow extrusion and sheetGlazing, machine guards, skylights and thick tough partsHard to fill thin injection parts; high melt temperature needed
Medium-flow clear injectionCovers, housings with windows, face shieldsWeld lines show in clear parts; plan gate location
High-flow and opticalLenses, light guides and thin-wall clear partsOptical grades need the tightest drying and clean handling; small specks show
UV-stabilized clearOutdoor glazing, lamp lenses, signageSlows yellowing; long outdoor service often still needs a hard coat or UV cap layer
Light-diffusingLED diffusers and light coversBalance light transmission against hiding the LEDs; ask for both values
FDA and medical clearFood-contact containers, device housings, fluid componentsAsk for the producer’s FDA letter; gamma sterilization yellows standard grades, so ask for a gamma-stable grade if needed. Alkaline dishwasher detergents, ammonia and amines attack PC, and long exposure to water above about 60°C / 140°F hydrolyzes it, so check the wash and use conditions

Typical starting points. Grades vary, so confirm on the data sheet for the exact grade.

Processing notes

  • Drying. Dry at about 120°C / 248°F for 2–4 hours. Target 0.02% or less; some optical and lighting programs set a tighter in-house limit, around 0.01%. Clear parts show splay that an opaque color would hide. See the drying chart for other resins.
  • Melt temperature. About 280–320°C / 536–608°F. Use the low end for thick sheet and the upper end for thin optical parts. Long residence at high melt temperature yellows the part, so keep residence within the grade sheet’s limit.
  • Mold temperature. About 70–120°C / 158–248°F. Hotter molds reduce molded-in stress, which in a clear part shows as rainbow patterns under polarized light.
  • Shrinkage. About 0.5–0.75% and close to the same in both directions, which helps lenses hold their shape.
  • Regrind. Optical parts often run little or none. For non-optical clear parts, keep regrind clean, dry and well below the roughly 20% some producer guides allow, and watch yellowness.
  • Most common defect. Black specks and yellowing from degraded material on screw and check ring. Purge with clean clear PC before a clear run, and keep color changes away from clear tools. See black specks and heat discoloration.

What to put on the purchase order

  • Melt flow at 300°C / 1.2 kg with an allowed range, plus notched Izod if the part is a guard or shield.
  • Optical values that matter to you: light transmission, haze and yellowness index. Ask which of them the producer reports on each lot.
  • Tint: water clear or the producer’s standard clear, which often has a slight blue tint. Two “clear” grades can look different side by side.
  • UV stabilization yes or no, and release agent yes or no.
  • Food or medical use: ask for the producer’s FDA letter for the exact grade, and say if the part must be BPA-free (standard PC cannot meet that).
  • Flame rating, if needed, with thickness. UL recognition is grade-specific and color-specific; check the grade’s listing on UL Product iQ.
  • Packaging and lots: sealed, moisture-barrier packaging, and a single lot for an optical program where possible.

When to consider something else

  • If clarity, scratch resistance and outdoor life matter more than impact, look at PC vs. acrylic.
  • If a clear outdoor part loses toughness in sunlight and some surface yellowing is acceptable, look at polyarylate.
  • If the clear part needs repeated steam sterilization or higher heat, look at polysulfone.
  • If the part is a low-cost clear item that will not be dropped or heated, look at polystyrene or SAN on the ASA / SAN page.
  • To compare all the clear options side by side, see best plastic for clear parts.

Common questions

Is polycarbonate food safe?

Some polycarbonate grades meet FDA food-contact requirements, but it depends on the exact grade, not the resin family. Ask for the producer’s FDA letter for that grade. In the U.S., FDA regulations no longer allow polycarbonate in baby bottles and sippy cups, and the EU now restricts BPA-based plastics in most food-contact uses. Standard PC is made from BPA, so it cannot meet a BPA-free requirement.

Does clear polycarbonate yellow in sunlight?

Yes, unstabilized polycarbonate yellows and its surface weakens outdoors, and it can start to show within a season or two. UV-stabilized grades slow this down. For long outdoor life, glazing and lenses usually also get a UV-resistant hard coat or a co-extruded UV cap layer.

Why are my clear polycarbonate parts yellow or full of black specks?

Usually the resin was overheated or sat too long in the barrel, or degraded material built up on the screw and check ring and is flaking off. Wet resin adds splay. Lower residence time, check heater zones, purge with clean clear PC and dry to 0.02% or less.

How clear is polycarbonate compared with acrylic?

Clear polycarbonate typically transmits about 88–90% of visible light, depending on grade and thickness, against about 92% for acrylic. Acrylic also stays clear outdoors longer without a coating and resists scratches better. Polycarbonate is chosen when the clear part must survive impact.

Related pages (12)

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. We check it, and suggest a matched alternative if it is hard to get.
  3. We aim to quote within one to three business days, from one gaylord to a railcar.
Rather talk? Call (678) 310-6899 or text a photo.
Quote request · Clear Polycarbonate

Tell us the Clear Polycarbonate grade you run now

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

Not sure? Just tap through 4 questions4 quick questions, then a chemist suggests a short list.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote