Surplus lotPrime PBT/PET, 55% glass, from a canceled auto program.120,000 lb PBT/PET 55% glass. See the lot
Plastic resin supply for the U.S. and Canada · Mon–Fri, 8am–5pm ET
Home › Materials › Carbon-filled nylon & PP

Carbon-filled nylon & polypropylene: stiffer and lighter than glass-filled, with static control by grade

We supply carbon-filled nylon 6 and 66, and carbon-filled polypropylene. Other base resins depend on availability, so ask.

One gaylord to a truckload · Every prime lot from our suppliers ships with a COA

Request a Quote
Shop-floor numbers

Shop-floor numbers

Drying
About 80°C / 176°F, 2–4 h
Melt temp
PA66 280–305°C · PA6 270–290°C
Mold temp
About 80–120°C / 176–248°F
Shrinkage
Lower along flow than glass; use the grade sheet
Watch for
Resistance out of range or uneven
Grades
Carbon-filled nylon 6 · Carbon-filled nylon 66 · Carbon-filled polypropylene

Typical values; confirm against the grade’s data sheet. One gaylord to a truckload · Supplier COA on every prime lot · Ships to the U.S. and Canada.

The short answer

Carbon-filled nylon and PP are for parts that need more stiffness per pound than glass gives, better wear, or a controlled static-dissipative or conductive surface. Choose the base resin for heat and chemistry, and the carbon type and loading for stiffness and resistance. The thing that most often goes wrong is ordering by fill percentage alone: a grade can meet the stiffness target and still read outside the resistance range on the molded part.

Grades we source

Tap a grade to add it to your quote request.

About carbon-filled resins

Carbon fiber raises stiffness and strength, cuts weight compared to glass-filled grades and improves wear. Conductive carbon (fiber, black or other forms) sets the electrical range, from static-dissipative to conductive by grade, so tell us the surface resistivity you need.

Nylon is the most common base. Polypropylene is a lower-cost option where heat and load are moderate. Send us the base resin, fill level and what the part has to do, and we will price it or a matching grade.

Common applications

  • Gears, bushings and wear parts
  • Structural brackets replacing metal
  • Static-sensitive electronics handling
  • Automotive and under-hood components
  • Fuel-handling and ESD-safe parts

Typical properties

StiffnessHigh
WeightLower than glass-filled
Static controlDissipative to conductive, by grade
WearGood to excellent
Base resinsNylon 6, nylon 66, PP
Relative costModerate-high

Property ranges are general guidance and vary by grade and supplier; a polymer chemist reviews the spec against the data sheet and COA.

Which grade to ask for

Decide first whether carbon is there for stiffness, for static control, or for both.

Grade typeUse it forWatch out for
Carbon fiber nylon 66Stiff, light brackets and arms; wear parts that run warmLower elongation and often lower notched impact than a glass grade
Carbon fiber nylon 6Similar parts where surface finish and easier molding matterLoses more stiffness than PA66 once conditioned
Carbon fiber polypropyleneLower-cost stiff parts at moderate heat and load; chemical contactLess heat resistance and creep strength than nylon
Static-dissipative gradesElectronics trays, handling fixtures, housingsLow loadings may not reach the range; readings change with gate location and surface skin
Conductive grades (carbon fiber or carbon black)Grounding parts, fuel and powder handlingCarbon black lowers impact strength, and some grades leave marks on surfaces they rub
Carbon fiber + PTFE or graphiteGears, bushings, thrust washersPTFE is a PFAS; check customer, state and provincial restrictions

Typical starting points. Grades vary, so confirm on the data sheet for the exact grade.

Processing notes

  • Drying. Nylon grades dry like the base nylon: about 80°C / 176°F in a dehumidifying dryer, 2–4 hours for PA66 grades and 2–6 hours for PA6 grades. PP grades need only surface drying, but filled PP is more moisture-sensitive than unfilled: producer sheets give about 80–82°C / 176–180°F for 2–3 hours. See the drying chart for other resins.
  • Melt temperature. Set by the base resin. PA66 grades about 280–305°C / 536–581°F; PA6 grades about 270–290°C / 518–554°F. PP grades follow the polypropylene window on the grade sheet.
  • Mold temperature. Nylon grades about 80–120°C / 176–248°F. Carbon pulls heat out of the melt quickly, so a hot mold and fast fill help keep fibers off the surface.
  • Shrinkage. Usually lower along the flow than a glass grade at the same loading, so the warp pattern changes when you switch. Use the data sheet for the exact grade.
  • Regrind. Fibers break with every pass, and broken fibers carry less load and conduct less well. Set a limit and re-measure stiffness and resistance at that ratio.
  • Most common defect. Resistance that is out of range or varies across the part, caused by a resin-rich skin or fibers broken by high shear. Change injection speed, melt temperature or mold temperature one at a time and re-measure. Use hardened barrels and tool steel, because carbon fiber is abrasive.

What to put on the purchase order

  • Base resin, carbon type (fiber or black) and loading percentage.
  • The resistance range with units (ohms or ohms per square), the test method and the humidity the parts are conditioned at. Under current ESD standards, static-dissipative is 104 to below 1011 ohms.
  • Whether the value is checked on a test plaque or on your molded part. They often differ.
  • Stiffness target as flexural modulus, dry and, for nylon, conditioned.
  • Lubricant package for wear parts, and whether the part must be PFAS-free.
  • Whether recycled carbon fiber grades are acceptable.
  • COA values: filler content and moisture, plus resistivity if the producer reports it per lot.

When to consider something else

Common questions

Is carbon fiber nylon conductive?

It can be. Depending on the loading, carbon-filled nylon ranges from insulating to static-dissipative to conductive. Low loadings may not reach the dissipative range, so specify the resistance range, units and test method instead of assuming.

Does carbon-filled nylon need to be dried?

Yes. The carbon does not absorb water, but the nylon does. Dry at about 80°C / 176°F in a dehumidifying dryer before molding, 2–4 hours for PA66 grades and 2–6 hours for PA6 grades, the same as the base nylon.

What surface resistance does a static-dissipative part need?

Current ESD standards treat 104 to below 1011 ohms as static-dissipative and below 104 ohms as conductive. Older specs quote surface resistivity in ohms per square, and exact limits vary by standard. Get the range, units and test method from your customer in writing.

When is carbon-filled PP a better choice than carbon-filled nylon?

When heat and load are moderate, the part sees chemicals that attack nylon, or cost matters more than maximum stiffness. PP absorbs almost no water, so it does not lose stiffness in humid air, but it creeps more and takes less heat than nylon.

Related pages (9)

Talk to a polymer chemist

Have a grade on a print, a bag label, or just a part you need to make? Send what you have.

  1. Send the grade, a callout or a photo of the bag label.
  2. We check it, and suggest a matched alternative if it is hard to get.
  3. We aim to quote within one to three business days, from one gaylord to a railcar.
Rather talk? Call (678) 310-6899 or text a photo.

Tell us the grade you run now

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

Not sure? Just tap through 4 questions4 quick questions, then a chemist suggests a short list.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to ZIP or postal code
Text usRequest a Quote