Carbon-Filled Nylon vs. Glass-Filled Nylon

Both fillers make nylon stiffer and stronger. Glass does it cheaply; carbon fiber does it with less weight and adds electrical conductivity.

The short answer

Use glass-filled nylon for most structural parts: it is lower cost, widely stocked, colorable and electrically insulating. Use carbon-filled nylon when you need more stiffness per pound, static dissipation or conductivity, or lighter parts, and the higher cost is justified. At the same fill level carbon is noticeably stiffer, but it is black only and conducts electricity.

Side by side

PropertyCarbon-Filled NylonGlass-Filled Nylon
StiffnessHigher at the same fillHigh
WeightLighter for the same stiffnessHeavier
Static controlDissipative to conductive, depending on carbon loading; low loadings may not reach the ESD range, so specify the resistivity you needInsulating
Wear against mating partsGenerally gentlerMore abrasive
ColorBlack onlyNatural, black or colored
Relative costHigherLower

Typical, general comparisons. Individual grades vary; check the data sheet.

Choose Carbon-Filled Nylon when

  • Maximum stiffness for the weight
  • Static dissipation (ESD) is needed
  • Better wear behavior in moving parts

Choose Glass-Filled Nylon when

  • Cost is the priority
  • You need color or electrical insulation
  • High-volume structural parts
Related pages (6)

Why they differ

The nylon is the same; the fiber does the work. Glass fiber has a density of about 2.5–2.6 g/cm³. Standard carbon fiber is about 1.75–1.8 g/cm³ and roughly three times stiffer than glass fiber. So at the same weight percent, carbon adds more stiffness and less weight.

In practice, a 30% glass PA66 runs about 1.36–1.39 g/cm³ with flexural modulus about 8.5–10 GPa dry. A 30% carbon PA66 is lighter, around 1.26–1.30 g/cm³ on many data sheets, and often lists about 13–20 GPa dry. That stiffness usually comes with lower elongation, and often lower notched impact than the glass grade, so check toughness if the part takes impact.

Carbon also conducts electricity and heat. That is useful for static control and a problem in parts that must insulate. Both fillers sit in nylon, so both still absorb moisture and lose some stiffness once conditioned.

Processing differences

  • Drying. Same as the base nylon: about 80°C (176°F) for 2–4 hours in a dehumidifying dryer. See the drying guide.
  • Melt and mold temperature. Set by the base resin. For PA66 grades, melt about 280–305°C (536–581°F) and mold about 80–120°C (176–248°F). Carbon grades pull heat out of the melt faster, so a hot mold and fast fill help keep fibers off the surface.
  • Shrinkage. Glass PA66 GF30 shrinks about 0.5% along the flow and 1.1% across. Carbon grades usually shrink even less along the flow, so the warp pattern changes when you swap. Use the data sheet values for the exact grade.
  • Wear on equipment. Both fillers wear screws, check rings and gates. Use hardened or bimetallic barrels and wear-resistant tool steel for either.
  • Regrind. Fiber breaks every time it is reground, which lowers strength and stiffness. Because carbon grades cost more, there is pressure to use more regrind; set a limit and test it.

Cost and availability

Glass-filled PA6 and PA66 are offered from about 13% to 60% glass in natural, black and colors, flame-retardant and heat-stabilized versions, by many producers. Carbon-filled nylon costs several times more per pound, has fewer grades, and longer lead times are common. Recycled-carbon-fiber grades exist and can narrow the cost gap. Because carbon is stiffer, a lower carbon loading can sometimes match a higher glass loading; compare at equal stiffness, not equal fill.

Common mistakes when switching

  • Assuming any carbon-filled grade is ESD safe. Low loadings may not reach the dissipative range; specify surface or volume resistivity. See static and ESD.
  • Putting a conductive carbon grade in a housing or bracket that must insulate.
  • Running a carbon grade in a tool cut for glass and expecting the same dimensions.
  • Letting carbon-filled parts touch aluminum in wet or salty service without isolation. Carbon can promote galvanic corrosion of the aluminum.
  • Forgetting the color: carbon grades are black only.

More: carbon-filled resins, glass-filled nylon, PA66 GF30 typical properties and glass-filled plastics explained.

Common questions

Is carbon fiber nylon stronger than glass-filled nylon?

It is stiffer at the same fill level, often 1.5–2 times the flexural modulus of a glass grade, and lighter. Tensile strength is often higher too, but impact and elongation are usually lower, so check the data sheet for the property that matters.

Is carbon-filled nylon conductive?

It can be. Depending on the carbon loading it ranges from insulating to dissipative to conductive, so specify the resistivity you need instead of assuming.

Can glass-filled nylon replace carbon-filled nylon?

Often, if the part does not need static control and can accept more weight or a higher glass loading for the same stiffness. Check dimensions and warp, because shrinkage differs.

Do carbon and glass-filled nylon need drying?

Yes. Both are nylon and absorb moisture, so dry at about 80°C (176°F) for 2–4 hours in a dehumidifying dryer before molding.

Why is carbon-filled nylon only black?

Carbon fiber is black and opaque, so it cannot be colored. Glass-filled nylon can be supplied natural, black or in custom colors.