Home › Grade cross-reference › Elastollan C 65 A HPM
Grade lookup

Elastollan C 65 A HPM: specs and equivalent grades

BASF soft aromatic polyester TPU from the Elastollan HPM series, nominal 65 Shore A. Published data, sister grades to ask about, and how to request a quote from one gaylord.

Request a Quote

On allocation or need a second source? Get options from a chemist ›

The short answer

Elastollan C 65 A HPM is a soft thermoplastic polyurethane (TPU) from BASF, based on a polyester polyol, in BASF’s aromatic HPM (high performance material) series. BASF’s range chart lists it as C 65 A 15 HPM with a measured hardness of 67 Shore A (DIN ISO 48-4, 3 s), density 1.18 g/cm³ (DIN EN ISO 1183-1-A), tensile strength 37 MPa and elongation at break 950% (DIN 53504-S2). BASF describes the HPM series as having very good damping and rebound, high temperature resistance, improved setting behavior and good demolding. Grades to ask about include BASF’s own Elastollan C 70 A 15 HPM, C 60 A 15 HPM and 565 A 12 P. They are not identical, so compare the data sheets and run a trial before switching.

Also written as: Elastollan C 65 A 15 HPM (full code in BASF’s range chart), Elastollan C65A HPM, BASF C 65 A HPM. In BASF’s naming, C means a polyester base, 65 A the nominal Shore A hardness, the 1 a cylindrical or lentil-shaped granule, the 5 an added lubricant, and HPM the high performance material series. Do not confuse it with Elastollan A C 65A 12 HPM, which BASF lists as an aliphatic polyester grade (color-fast, non-yellowing). Quote the full code from your drawing or bag label.

Buying Elastollan C 65 A HPM: one gaylord to a railcar · supplier COA on every prime lot · access to 100+ partner warehouse locations · a polymer chemist checks the grade code before we quote · we aim to quote within one to three business days

Quick quote

Have a part number or drawing callout?

Paste it as written. A polymer chemist will tell you which grade it calls for, suggest close alternatives to qualify and quote it by email.

No account needed · No obligation · Orders from one gaylord · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

Elastollan C 65 A HPM specs from the data sheet

Typical values from BASF’s Elastollan product range chart (HPM series page). BASF notes these are typical values; the full product information and processing guidance for the grade should be checked before use. The lot COA shows what you actually receive. Values only compare at the same test method and condition.

PropertyValueTest method or note
Producer (brand owner)BASF (BASF Polyurethanes GmbH; Elastollan is a registered trademark of BASF SE)BASF range chart
PolymerThermoplastic polyurethane, aromatic, polyester based (TPU-ARES); HPM seriesBASF range chart; Material Data Center classification
Hardness67 Shore A (nominal 65 A)DIN ISO 48-4, 3 s
Density1.18 g/cm³DIN EN ISO 1183-1-A
Tensile strength37 MPaDIN 53504-S2
Elongation at break950%DIN 53504-S2
Stress at 20% / 100% / 300% elongation1.5 / 2 / 4 MPaDIN 53504-S2
Tear strength44 kN/mDIN ISO 34-1, method B(b)
Abrasion loss55 mm³DIN ISO 4649-A
Compression set25% at 23°C / 72 h; 37% at 70°C / 24 h; 55% at 100°C / 24 hDIN EN ISO 815-1
After 21 days in water at 80°CTensile strength 35 MPa; elongation at break 900%DIN 53504-S2
Notched Charpy impact, +23°C and -30°CNo breakDIN EN ISO 179-1
Vicat softening temperature80°CDIN EN ISO 306, 10 N, 120°C/h (A120)
Melt flowNot published in the BASF range chartAsk for the grade product information
DryingDry granules to below 0.02% moisture before processing. BASF’s drying table for the HPM product range: 3–5 hours at 60–80°C in dehumidified air; circulating-air drying is listed as not suitable.BASF Elastollan processing recommendations
Melt and mold temperatureNot published in the BASF sources we could openAsk for the grade product information
Food contactNo food-contact statement for this grade in the range chart. BASF lists separate FC grades for food contact.BASF range chart

Source data sheets are listed at the bottom of this page. Confirm against the current sheet for your exact grade code and color.

BASF’s test plaques for Elastollan are injection molded and tested at standard lab conditions; hardness, tear and compression set depend on dwell time, specimen type and conditioning, so compare them only at the same method.

Grades to ask about instead of Elastollan C 65 A HPM

These grades have similar published specs. All three are BASF aromatic polyester TPUs, so the polymer type matches. None is a drop-in replacement: hardness, additive packages, flow at processing shear rates, color and approvals differ. If your part, drawing or customer approval names Elastollan C 65 A HPM, any change needs your approval and usually a trial.

GradeProducerMelt flowDensityKey propertyHow it compares
Elastollan C 70 A 15 HPMBASFNot published in the range chart1.18 g/cm³ (DIN EN ISO 1183-1-A)71 Shore A (DIN ISO 48-4, 3 s); tensile 40 MPa, elongation 900% (DIN 53504-S2); tear 45 kN/m; abrasion 50 mm³; Vicat 90°CCheck. Same HPM polyester series, one step harder (71 vs. 67 Shore A measured). Slightly stronger, higher Vicat and lower compression set at 70°C (35% vs. 37%). Same density. A part designed around 65 A will feel stiffer. Quote this alternative ›
Elastollan C 60 A 15 HPMBASFNot published in the range chart1.17 g/cm³ (DIN EN ISO 1183-1-A)63 Shore A (DIN ISO 48-4, 3 s); tensile 20 MPa, elongation 1,000% (DIN 53504-S2); abrasion 98 mm³; Vicat 70°CCheck. Same HPM polyester series, one step softer. Much lower tensile strength (20 vs. 37 MPa), almost twice the abrasion loss and a lower Vicat, so it suits softer parts with less wear. Quote this alternative ›
Elastollan 565 A 12 PBASFNot published in the range chart1.22 g/cm³ (DIN EN ISO 1183-1-A)66 Shore A (DIN ISO 48-4, 3 s); tensile 30 MPa, elongation 850% (DIN 53504-S2); tear 65 kN/m; abrasion 55 mm³Partial match. Aromatic polyester TPU from BASF’s 500 series at a similar hardness, but not an HPM grade. BASF’s code P means it contains plasticizer, which can matter for migration, bonding and long-term hardness. Denser, so part weight changes. Quote this alternative ›

From BASF’s published range chart. Brand owners and grade names change; confirm on the current data sheet. We have not listed TPUs from other producers here because we could not confirm matching published data for them; ask and a chemist will compare current sheets.

Typical uses for Elastollan C 65 A HPM

BASF’s range chart describes the HPM series as offering:

  • Very good damping behavior and rebound
  • High temperature resistance
  • Improved setting behavior
  • Good demolding properties

BASF’s range chart does not list specific end uses for C 65 A HPM. BASF does use it as the soft polyester example in its Elastollan material properties brochure (torsion modulus and damping, stress-strain at temperature, tear strength vs. temperature and thermal expansion curves), which is a useful reference if you are designing a soft damping or sealing part. For the TPU family in general, see our TPU buying guide.

What to check before you switch

  • Hardness: the name says 65 A, but BASF’s chart gives 67 Shore A at a 3 s reading. Compare any alternative at the same scale, dwell time and specimen type.
  • Aromatic vs. aliphatic: Elastollan A C 65A 12 HPM is a different, aliphatic polyester grade for color-fast, non-yellowing parts. Check which one your print calls for.
  • Polyester vs. polyether: BASF lists hydrolysis resistance and resistance to microorganisms for its polyether (11 series) grades, not for the C series. C 65 A HPM kept 35 of 37 MPa tensile after 21 days in 80°C water in BASF’s test, but for long hot-water or humid service compare a polyether TPU. See TPE vs. TPU.
  • Seals and buffers: compare compression set at the same temperature and time. C 65 A HPM is 25% at 23°C but 55% at 100°C. See seal compression set.
  • Drying: TPU is hygroscopic. Dry to below 0.02% moisture; for HPM grades BASF gives 3–5 hours at 60–80°C in dehumidified air, not a circulating-air dryer. Dry any color masterbatch with the resin. See the resin drying guide.
  • Plasticizer: 565 A 12 P contains plasticizer; C 65 A HPM is not marked P. Check bonding, paint and contact with other parts before switching.
  • Availability: the range chart does not say where the grade is made or sold. Lead time is confirmed with your quote.
  • Run a trial lot and check hardness, shrinkage, demolding and surface before you switch production.

Need a second source for Elastollan C 65 A HPM?

Tell us why. A polymer chemist will reply with one to three alternatives, what differs, and what to test before you switch. Free.

No obligation. Privacy

Watch Elastollan C 65 A HPM

Get a short email only if Elastollan C 65 A HPM changes owner, is renamed or discontinued, goes on allocation, gets a price increase, or when a matching surplus lot comes in. Free. Add your other grades too.

Stop anytime: reply “stop” to any alert. Privacy

Buying Elastollan C 65 A HPM: price, lead time and lot size

  • Lot size. From one gaylord to a railcar. See gaylord, LTL and truckload for typical weights per box.
  • Where it ships from. We have access to 100+ partner warehouse locations. Material already in a partner warehouse usually moves sooner than a grade that has to come from the producer; your quote says which applies.
  • Price. We do not publish prices because they move with feedstock, freight and order size. What moves your price most: lot size, color, ship-to region, whether the grade has to come from overseas, and whether you need Elastollan C 65 A HPM itself or can accept a matched alternative. See how resin is priced and the monthly market update.
  • Paperwork. Supplier COA on every prime lot (what a COA shows). Ask for BASF’s product information sheet and any regulatory statement your part needs.
  • Trying an alternative? Start with one gaylord as a trial lot, molded and checked before you commit a full release. Samples (~50 lb) are available upon credit approval.
  • If Elastollan C 65 A HPM itself is not available. Some branded grades are sold only through the producer’s own channels or go on allocation. If we cannot source it, we tell you, then quote a matched alternative with a side-by-side comparison.

Send the grade code, your annual volume and ship-to location. A polymer chemist checks it before we quote; we were founded by a family with 30+ years in the resin business. For several grades at once, use the resin RFQ template.

Trade names belong to their owners. ResinBridge is not affiliated with these producers; grade names are used only to identify the material. Data reflects published sheets as of November 2026.

Sources

Common questions

What is Elastollan C 65 A HPM?

Elastollan C 65 A HPM is a soft, aromatic, polyester-based thermoplastic polyurethane (TPU) from BASF in its HPM (high performance material) series. BASF describes the HPM series as having very good damping and rebound, high temperature resistance, improved setting behavior and good demolding.

What is the hardness of Elastollan C 65 A HPM?

The nominal hardness is 65 Shore A. BASF’s range chart lists the measured value for C 65 A 15 HPM as 67 Shore A (DIN ISO 48-4, 3 s reading).

Is Elastollan C 65 A HPM polyester or polyether?

Polyester. In BASF’s naming, the C series is polyester based, and Material Data Center classifies C 65 A HPM as TPU-ARES (aromatic polyester TPU).

Is C 65 A HPM the same as Elastollan A C 65A 12 HPM?

No. BASF lists A C 65A 12 HPM as an aliphatic polyester grade aimed at color-fast, non-yellowing parts. C 65 A HPM is aromatic. Check the full code on your drawing or bag label.

What is equivalent to Elastollan C 65 A HPM?

The closest grades to ask about are BASF’s own Elastollan C 70 A 15 HPM (harder) and C 60 A 15 HPM (softer, weaker), plus 565 A 12 P, a plasticized polyester TPU at 66 Shore A. None is identical; compare data sheets and run a trial, and get approval if your part names C 65 A HPM.

Does Elastollan C 65 A HPM need drying?

Yes. BASF says Elastollan is hygroscopic and should be dried to below 0.02% moisture before processing. For the HPM product range, BASF’s drying table gives 3–5 hours at 60–80°C in a dehumidified-air dryer and lists circulating-air drying as not suitable.

Can ResinBridge supply Elastollan C 65 A HPM?

We quote Elastollan C 65 A HPM when our supply partners can source it. If they cannot, we say so up front and quote a matched alternative, named on the quote with its data sheet, so you can decide whether to trial it.

If your grade is not listed, tell us what you run. We source commodity, engineering and specialty resins.

Need Elastollan C 65 A HPM or an alternative to qualify?

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

ResinBridge is not an authorized distributor of Elastollan; when we source Elastollan C 65 A HPM through our supply network, we confirm lot origin and COA with your quote.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until the order is confirmed in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to city and state or province

Quote Elastollan C 65 A HPM or a matched alternative

A polymer chemist checks the data sheet and tells you exactly what you would get before you order.

Request a Quote

Not sure which grade fits your part?

Send the grade you run now, or describe the part.

Text usRequest a Quote