Home › Grade cross-reference › Dow DMDA-8007 NT 7
Grade lookup

Dow DMDA-8007 NT 7: specs and equivalent grades

Dow narrow molecular weight distribution HDPE homopolymer for injection molded crates, cases, trays and totes, and cast film. Published data, grades from other producers to ask about, and how to request a quote from one gaylord.

Request a Quote

The short answer

Dow DMDA-8007 NT 7 is Dow's narrow molecular weight distribution high density polyethylene homopolymer for injection molded crates, cases, trays and tote bins. Dow says it is also suitable for cast film. Dow's technical data sheet gives a melt index of 8.3 g/10 min, measured at 190°C / 374°F, 2.16 kg, ASTM D1238, and density of 0.965 g/cm³ (ASTM D792). Grades from other producers to ask about include Alathon M6580, Marlex 9708, SCLAIR 2908 and Formolene LH6008. They are not identical, so compare the data sheets and run a trial before switching.

Also written as: DOW HDPE DMDA-8007 NT 7, DOW DMDA-8007 NT 7. Quote the full code from your drawing or bag label; color and additive suffixes change the grade.

Buying Dow DMDA-8007 NT 7: one gaylord to a railcar · supplier COA on every prime lot · ships from 22+ partner warehouse locations · a polymer chemist checks the grade code before we quote · we aim to quote within one to three business days

Quick quote

Have a part number or drawing callout?

Paste it as written. A polymer chemist will tell you which grade it calls for, suggest equivalents and quote it by email.

No account needed · No obligation · Orders from one gaylord · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

Dow DMDA-8007 NT 7 specs from the data sheet

Typical values from Dow's technical data sheet (form 410-362-01-0725, issued for North America, Latin America and Asia Pacific) and Dow's product page. Molded properties were tested per ASTM D4976. Typical values are not specifications; the lot COA shows what you actually receive. Values only compare at the same test method and condition.

PropertyValueTest method or note
Producer (brand owner)DowDow product page and technical data sheet
PolymerHigh density polyethylene homopolymer, narrow molecular weight distributionDow technical data sheet
ProcessInjection molding; cast film extrusion
Melt flow8.3 g/10 min190°C / 374°F, 2.16 kg, ASTM D1238
High load melt index180 g/10 min190°C / 374°F, 21.6 kg, ASTM D1238
Density0.965 g/cm³ASTM D792
ESCR2 h50°C, 100% Igepal, F50, ASTM D1693
Tensile strength, yield / break31.0 / 17.9 MPa (4,500 / 2,600 psi)ASTM D638
Tensile elongation, yield / break6 / 350 %ASTM D638
Flexural modulus, 2% secant1,410 MPa (205,000 psi)ASTM D790B
Tensile impact strength168 kJ/m² (80.0 ft-lb/in²)ASTM D1822
HardnessShore D 61ASTM D2240
HDT 0.45 MPa (66 psi), unannealed83.9°C / 183°FASTM D648
Brittleness temperatureBelow −76.1°C (−105°F)ASTM D746
Vicat softening temperature131°C / 268°FASTM D1525
Melting temperature133°C / 271°FDSC, Dow method
Benefits stated by DowExcellent stiffness and modulus, excellent warp resistance, high gloss, low odorDow product page
AdditivesNo antiblock, slip or processing aidDow technical data sheet
Food contactDow's technical data sheet states it complies with U.S. FDA 21 CFR 177.1520 (c)2.2, has a Canadian HPFB No Objection and complies with EU No 10/2011, and says to consult the regulations for complete details. Ask Dow for its current letter.
Injection molding melt and mold temperatureNot published on the data sheetDow TDS form 410-362-01-0725 gives no injection molding settings
Cast film fabrication conditions (Dow test film)Melt 500°F (260°C); chill roll 70°F (21°C); 36 in (914 mm) die, 25 mil (0.6 mm) die gap; 400 fpm (123 m/min); 426 lb/hrDow TDS 410-362-01-0725, Extrusion Notes. Conditions used to make the 1 mil test film, not a recommendation. The notes print 261°C for 500°F; the property table prints 260°C
DryingNot published on the data sheetDow TDS 410-362-01-0725
Packaging formsNot published on the data sheetDow TDS and product page

Source data sheets are listed at the bottom of this page. Confirm against the current sheet for your exact grade code and color.

The producer's sheet gives no drying step; PE and PP do not normally need drying, but material moved from a cold warehouse into a warm plant can pick up surface condensation, so let it reach room temperature in the closed box before opening.

Grades to ask about instead of Dow DMDA-8007 NT 7

These grades from other producers have similar published specs. None is a drop-in replacement: additive packages, flow at molding shear rates, color and approvals differ. If your part, drawing or customer approval names Dow DMDA-8007 NT 7, any change needs your approval and usually a trial.

GradeProducerMelt flowDensityKey propertyHow it compares
Alathon M6580LyondellBasell8.2 g/10 min (190°C / 374°F, 2.16 kg, ASTM D1238)0.965 g/cm³ (ASTM D1505)Flexural modulus, 1% secant 1,650 MPa (240,000 psi) (ASTM D790); notched Izod 36 J/m (ASTM D256)Close match. Narrow molecular weight distribution homopolymer for cases, crates, trays, tote bins and open-head pails; North America. Same density, MFR within about 1%. Regulatory details are in LyondellBasell's Product Stewardship Bulletin, a separate document. Quote this alternative ›
Marlex 9708Chevron Phillips Chemical8.0 g/10 min (190°C / 374°F, 2.16 kg, ASTM D1238)0.962 g/cm³ (ASTM D1505)Flexural modulus, tangent 1,580 MPa (230,000 psi) (ASTM D790); notched Izod 40 J/m (0.8 ft-lb/in) (ASTM D256)Close match on use. Injection molding HDPE for crates, tote boxes and structural foam; ESCR < 10 h (Condition B, 100% Igepal). CPChem states FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H. CPChem describes it as an ethylene homopolymer; density is slightly lower. Quote this alternative ›
SCLAIR 2908NOVA Chemicals7.0 g/10 min (190°C / 374°F, 2.16 kg, ASTM D1238)0.961 g/cm³ (ASTM D792)Flexural modulus 1,280 MPa (185,600 psi) (ASTM D790); ESCR F50 < 10 h (ASTM D1693)Partial match. Homopolymer HDPE injection resin for tote boxes and beverage crates. MFR about 16% lower and lower published stiffness. NOVA states FDA 21 CFR 177.1520 (c) 2.2. Quote this alternative ›
Formolene LH6008Formosa Plastics USA8.0 g/10 min (190°C / 374°F, 2.16 kg, ASTM D1238)0.965 g/cm³ (ASTM D1505)Flexural modulus, 2% secant 1,550 MPa (225,000 psi) (ASTM D790B); ESCR 2 h (100% Igepal, 50°C, F50, ASTM D1693)Close match. Homopolymer HDPE injection resin for industrial crates, totes and bins and small appliances. Same density, MFR within about 4%. Formosa states it meets FDA 21 CFR 177.1520. Quote this alternative ›

From each producer's published data. Brand owners and grade names change; confirm on the current data sheet.

Typical uses for Dow DMDA-8007 NT 7

From Dow's product page and technical data sheet:

  • Crates
  • Cases
  • Trays
  • Tote bins
  • Hygiene non-breathable backsheet films

What to check before you switch

  • Flexural modulus is reported differently: Dow and Formosa give a 2% secant value (ASTM D790B), LyondellBasell gives 1% secant and CPChem gives tangent modulus, so the numbers do not compare directly.
  • Narrow molecular weight homopolymers trade stress-crack resistance for stiffness: Dow lists ESCR of 2 h for DMDA-8007 NT 7 (50°C, 100% Igepal, F50), and the alternatives list 2 h (LH6008) and < 10 h (Marlex 9708, SCLAIR 2908). Do not use them for stress-crack-critical parts without testing.
  • Density is measured by ASTM D792 for Dow and NOVA and by ASTM D1505 for LyondellBasell, CPChem and Formosa.
  • Dow's data sheet states FDA, Canadian HPFB and EU compliance for DMDA-8007 NT 7; get Dow's current regulatory letter for your file.
  • NT 7 is part of Dow's grade name. Quote and approve against the full name, DMDA-8007 NT 7.
  • Compare melt flow, density and impact only at the same test condition and method (ASTM vs. ISO results differ).
  • Ask for the producer's food-contact or regulatory letter for the exact grade if the part needs one.
  • Run a trial lot and check shrinkage, cycle time and appearance before you switch production.

Buying Dow DMDA-8007 NT 7: price, lead time and lot size

  • Lot size. From one gaylord to a railcar. See gaylord, LTL and truckload for typical weights per box.
  • Where it ships from. 22+ partner warehouse locations. Material already in a partner warehouse usually moves sooner than a grade that has to come from the producer; your quote says which applies.
  • Price. We do not publish prices because they move with feedstock, freight and order size. What moves your price most: lot size, color, ship-to region, and whether you need Dow DMDA-8007 NT 7 itself or can accept a matched alternative. See how resin is priced and the monthly market update.
  • Paperwork. Supplier COA on every prime lot (what a COA shows). Ask for the producer’s regulatory letter or UL file if your part needs them.
  • Trying an alternative? Start with one gaylord as a trial lot, molded and checked before you commit a full release.
  • If Dow DMDA-8007 NT 7 itself is not available. Some branded grades are sold only through the producer’s own channels or go on allocation. If we cannot source it, we tell you, then quote a matched alternative with a side-by-side comparison.

Send the grade code, your annual volume and ship-to location. A polymer chemist checks it before we quote; we have been in the resin business for 30+ years. For several grades at once, use the resin RFQ template.

Trade names belong to their owners. ResinBridge is not affiliated with these producers; grade names are used only to identify the material. Data reflects published sheets as of October 2026.

Sources

Common questions

What is Dow DMDA-8007 NT 7?

Dow DMDA-8007 NT 7 is Dow's narrow molecular weight distribution high density polyethylene homopolymer for injection molded crates, cases, trays and tote bins. Dow says it is also suitable for cast film.

What is the melt flow of Dow DMDA-8007 NT 7?

8.3 g/10 min (melt index), measured at 190°C / 374°F, 2.16 kg, ASTM D1238, per Dow's technical data sheet. High load melt index is 180 g/10 min at 190°C, 21.6 kg.

What is equivalent to Dow DMDA-8007 NT 7?

Grades from other producers to ask about include Alathon M6580, Marlex 9708, SCLAIR 2908 and Formolene LH6008. None is identical; compare data sheets and run a trial, and get approval if your part names Dow DMDA-8007 NT 7.

Is Dow DMDA-8007 NT 7 food-contact compliant?

Dow's technical data sheet states it complies with U.S. FDA 21 CFR 177.1520 (c)2.2, has a Canadian HPFB No Objection and complies with EU No 10/2011, and says to consult the regulations for complete details. Ask Dow for its current regulatory letter for your file.

Can ResinBridge quote Dow DMDA-8007 NT 7?

Yes. Send the grade name and volume. A polymer chemist checks it and we quote the grade where we can source it, or a matched alternative, and say which one. Orders start at one gaylord; U.S. and Canada only.

If your grade is not listed, tell us what you run. We source commodity, engineering and specialty resins.

Need Dow DMDA-8007 NT 7 or an equivalent?

A polymer chemist reviews every request, then matches your grade or finds a matched alternative and prices it.

No account needed · No obligation · U.S. and Canada only · Orders from one gaylord
Quotes are not binding until we confirm your order in writing. Terms · Privacy

Faster: text a photo of your bag label to (678) 310-6899.

What to send for an accurate quote
  • The grade name, from any supplier, or a data sheet
  • Color (natural, black or a custom match)
  • Fill type and percentage, if any
  • Melt flow, if you know it
  • Quantity for this order and what you use in a year
  • Ship-to city and state or province

Quote Dow DMDA-8007 NT 7 or a matched alternative

A polymer chemist checks the data sheet and tells you exactly what you would get before you order.

Request a Quote

Not sure which grade fits your part?

Send the grade you run now, or describe the part.

Text usRequest a Quote